  "abstract": "The correct method for measuring Li (Na) diffusion coefficients has always been the subject of lengthy debates, due to the numerous approximations that can be used, resulting in large variations in reported values for the same material in the literature. This work first quantifies the limitations of the classical galvanostatic intermittent titration technique when applied to 2D or 3D diffusion, which are beyond the 1D case for which the technique was devised. Furthermore, to transition to powder-based electrodes the diffusion impedance of a log-normal particle size distribution (PSD) is considered. We introduce an equivalent diffusion length L eq for the PSD, corresponding to a time constant that can be estimated by electrochemical impedance spectroscopy. We applied this new method, which reliably estimates a diffusion coefficient by taking PSD into account, to determine the Li diffusivity in high-Ni NMC. Values ranging from 1.1 to 3.2 10 −11 cm 2 s −1 were found between 3.75 and 4.2 V vs Li + /Li. The time constant is easier to access than L eq , which is the main source of uncertainty and therefore requires meticulous evaluation. We hope that the battery community will consider adopting this approach to unify the reported diffusion coefficient values for existing and new electrode materials.",
  "abstract_shown": true,
  "affiliations": [],
  "article_type": null,
  "arxiv": null,
  "author_total": 6,
  "authors": [
    {
      "name": "Romain Dugas"
    },
    {
      "name": "Nicolas Murer"
    },
    {
      "name": "Cédric Boissière"
    },
    {
      "name": "Ronan Chometon"
    },
    {
      "name": "Gwenaëlle Rousse"
    },
    {
      "name": "Jean-Marie Tarascon"
    }
  ],
  "bibtex": "https://research.draconitic.com/paper/8cneysgce0per.bib",
  "cited_by": 0,
  "doi": "10.1149/1945-7111/ae94ef",
  "fulltext_url": null,
  "id": "8cneysgce0per",
  "issns": [
    "0013-4651",
    "1945-7111"
  ],
  "landing_url": "https://hal.sorbonne-universite.fr/hal-05863852v1",
  "language": "en",
  "licence": "CC-BY-4.0",
  "licence_label": "CC BY 4.0",
  "licence_source": "article",
  "licence_url": "https://creativecommons.org/licenses/by/4.0/",
  "metadata_licence": null,
  "native_subjects": [
    [
      "hal",
      "0.chim"
    ],
    [
      "openalex",
      "2208|Advancements in Battery Materials"
    ]
  ],
  "openalex": "W7172426026",
  "pdf_url": "https://hal.sorbonne-universite.fr/hal-05863852/document",
  "pmcid": null,
  "pmid": null,
  "published": "2026-08-27",
  "publisher": "Electrochemical Society / IOPscience",
  "ris": "https://research.draconitic.com/paper/8cneysgce0per.ris",
  "sources": [
    {
      "first_seen": "2026-11-15T12:20:47Z",
      "native_id": "hal-05863852",
      "source": "hal",
      "url": "https://hal.sorbonne-universite.fr/hal-05863852v1"
    }
  ],
  "subjects": [
    {
      "field": "chemistry",
      "origin": "hal:0.chim",
      "subfield": "general"
    }
  ],
  "title": "The Equivalent Diffusion Length in the Active Material of Powder-Based Electrodes",
  "title_text": "The Equivalent Diffusion Length in the Active Material of Powder-Based Electrodes",
  "type": "peer-reviewed",
  "updated_at": "2026-11-15T12:20:47Z",
  "url": "https://research.draconitic.com/paper/8cneysgce0per",
  "venue": "Journal of The Electrochemical Society",
  "versions": []
}