Skip to content
DraconiticResearch
Search Sources API
276,906 studies31 sourcesUpdated 41 min ago
Peer-reviewedCC BYRSC advances

Function-integrated injectable poly(methyl methacrylate) bone cement engineered with silver-templated mesoporous calcium-silicate nanoparticles via a chitosan-glycerophosphate hydrogel.

6 affiliations
  1. 1Department of Stomatology, Union Hospital, Tongji Medical College, Huazhong University of Science and Technology Wuhan 430022 China [email protected].
  2. 2School of Stomatology, Tongji Medical College, Huazhong University of Science and Technology Wuhan 430030 China.
  3. 3Hubei Province Key Laboratory of Oral and Maxillofacial Development and Regeneration Wuhan 430022 China.
  4. 4The State Key Laboratory Breeding Base of Basic Science of Stomatology (Hubei-MOST), Key Laboratory of Oral Biomedicine Ministry of Education, School & Hospital of Stomatology, Wuhan University 237 Luoyu Road Wuhan 430079 PR China [email protected].
  5. 5Department of Prosthodontics, Hospital of Stomatology, Wuhan University 237 Luoyu Road Wuhan 430079 PR China.
  6. 6Department of Prosthodontics, Wuhan Third Hospital(Tongren Hospital of WuHan University) Wuhan 430060 PR China.

Abstract

Polymethylmethacrylate (PMMA) bone cement remains a mainstay of bone reconstruction, yet its high polymerization exotherm, mismatched stiffness, bioinertness and lack of antibacterial activity can lead to thermal injury, stress shielding and post-operative infection. Here we report a single-phase strategy that addresses these limitations together. Mesoporous calcium-silicate nanoparticles (MCSNs) and silver-templated MCSNs (Ag-MCSNs) were dispersed in a thermosensitive chitosan-glycerophosphate (CS-GP) hydrogel and blended with PMMA to prepare three modified cements. The hydrogel phase lowered the peak polymerization temperature from ∼77 °C to below 40 °C, extended the working time beyond 20 min and created interconnected pores throughout the PMMA matrix with a dominant pore diameter of ∼79 µm. The modified cements exhibited an elastic modulus of 140-170 MPa and a compressive yield strength of 7-10 MPa, closely matching cancellous bone, and these properties were retained after 28 days of immersion in simulated body fluid. The MCSN-containing cements additionally promoted apatite deposition, with cumulative calcium uptake reaching 2.8-3.3 mmol L⁻¹ at day 28. Antibacterial testing against E. coli and S. aureus showed that only the Ag-MCSN cement produced clear inhibition zones, disrupted bacterial membranes on contact, and significantly reduced the number of recoverable colonies (p < 0.05) without compromising cytocompatibility. A single Ag-MCSN phase can therefore endow PMMA cement with combined bioactivity and antibacterial activity while improving its thermal and mechanical performance, a combination that holds promise for infection-resistant bone reconstruction.

Related

  1. Engineered injectable scaffolds as synthetic niches for minimally invasive monitoring of metastatic breast cancer progression
    Kathryn Kang, Grace K. Darlak, Jian Toy +8
    Bioengineering & translational medicinePeer-reviewedCC BYFull textMaterials & polymersEurope PMCPMC
  2. Injectable thermoresponsive hydrogel integrating pH-responsive nanoparticles for antioxidant therapy of intervertebral disc degeneration
    Yong Sun, Kun Wang, Yongjie Qiao +10
    Materials Today BioPeer-reviewedCC BY-NC 4.0Full textMaterials & polymersPMC
  3. Engineered nickel oxide nanoparticles impede mitochondrial function and compromise TCA cycle in Allium cepa L.
    Indrani Manna, Debalina Das, Maumita Bandyopadhyay
    Physiology and Molecular Biology of PlantsPeer-reviewedLicence not statedFull textMaterials & polymersPMC
  4. Surface-Engineered 3D-Printed Polymeric Flat-Panel Photoreactors with P25 TiO2 Nanoparticles for Photocatalytic Hydrogen Evolution
    María José Torres, Jesús Román, María del Prado Garrido +1
    NanomaterialsPeer-reviewedCC BY 4.0Materials & polymersCrossref
  5. From Design to Bedside: Brain-Targeted Engineered Nanoparticles and Predictive Modeling for Neurodegenerative Diseases Therapeutics
    Nguyen Nguyen, Muzhaozi Yuan, Ya Wang
    Pharmaceutical ResearchPeer-reviewedCC BY 4.0Full textMaterials & polymersPMC
BibTeX
@article{zhao2026functionintegrated,
  title = {{Function-integrated injectable poly(methyl methacrylate) bone cement engineered with silver-templated mesoporous calcium-silicate nanoparticles via a chitosan-glycerophosphate hydrogel.}},
  author = {Xuan Zhao and Ping Li and Yue Sa and Man Wang},
  journal = {RSC advances},
  year = {2026},
  month = nov,
  doi = {10.1039/d6ra08568g},
  url = {https://europepmc.org/article/MED/43075552},
  note = {CC BY},
}
RIS
TY  - JOUR
TI  - Function-integrated injectable poly(methyl methacrylate) bone cement engineered with silver-templated mesoporous calcium-silicate nanoparticles via a chitosan-glycerophosphate hydrogel.
AU  - Xuan Zhao
AU  - Ping Li
AU  - Yue Sa
AU  - Man Wang
PY  - 2026
DA  - 2026/11/23
JO  - RSC advances
DO  - 10.1039/d6ra08568g
UR  - https://europepmc.org/article/MED/43075552
AB  - Polymethylmethacrylate (PMMA) bone cement remains a mainstay of bone reconstruction, yet its high polymerization exotherm, mismatched stiffness, bioinertness and lack of antibacterial activity can lead to thermal injury, stress shielding and post-operative infection. Here we report a single-phase strategy that addresses these limitations together. Mesoporous calcium-silicate nanoparticles (MCSNs) and silver-templated MCSNs (Ag-MCSNs) were dispersed in a thermosensitive chitosan-glycerophosphate (CS-GP) hydrogel and blended with PMMA to prepare three modified cements. The hydrogel phase lowered the peak polymerization temperature from ∼77 °C to below 40 °C, extended the working time beyond 20 min and created interconnected pores throughout the PMMA matrix with a dominant pore diameter of ∼79 µm. The modified cements exhibited an elastic modulus of 140-170 MPa and a compressive yield strength of 7-10 MPa, closely matching cancellous bone, and these properties were retained after 28 days of immersion in simulated body fluid. The MCSN-containing cements additionally promoted apatite deposition, with cumulative calcium uptake reaching 2.8-3.3 mmol L⁻¹ at day 28. Antibacterial testing against E. coli and S. aureus showed that only the Ag-MCSN cement produced clear inhibition zones, disrupted bacterial membranes on contact, and significantly reduced the number of recoverable colonies (p < 0.05) without compromising cytocompatibility. A single Ag-MCSN phase can therefore endow PMMA cement with combined bioactivity and antibacterial activity while improving its thermal and mechanical performance, a combination that holds promise for infection-resistant bone reconstruction.
SN  - 2046-2069
ER  -