Cu-modified ZnO nanostructures on 3D-printed photopolymer scaffolds for reusable photocatalytic degradation of methylene blue
- 1Izmir Katip Celebi University, Dept. of Metallurgical and Materials Engineering Izmir 35620 Turkey
Abstract
Cu-modified ZnO nanostructures were hydrothermally grown on three-dimensional epoxy/acrylate photopolymer scaffolds fabricated by LCD-based vat photopolymerization. After surface activation and ZnO seed-layer deposition, coatings with nominal Cu contents of 0.5, 1, and 2 wt% were grown at 90 °C for 4 h. X-ray diffraction and Raman spectroscopy confirmed preservation of hexagonal wurtzite ZnO, while Cu addition modified the principal diffraction reflections without detectable secondary Cu-containing crystalline phases. Electron microscopy and elemental analysis revealed dense rod-like nanostructures with Cu-dependent morphology and verified Cu in the coatings. Optical measurements showed Cu-dependent changes in reflectance, band-gap energy, and defect-related emission. After 180 min under artificial sunlight, the mean methylene blue (MB) degradation efficiency increased from (54.59 ± 1.61)% for ZnO/P to (83.67 ± 1.08)% for 2Cu–ZnO/P. The latter exhibited an apparent rate constant of (8.78 ± 0.39) × 10−3 min−1, approximately 2.2 times that of ZnO/P. Scavenger experiments indicated a predominant role of superoxide radicals under the investigated conditions. One of the three 2Cu–ZnO/P scaffolds was used for four additional cycles. Its MB degradation efficiency decreased from 84.88% in cycle 1 to 78.11% in cycle 5, corresponding to 92.02% retention of its first-cycle efficiency. These results demonstrate the potential of Cu-modified ZnO on open cubic vertex-centroid scaffolds as reusable immobilized photocatalysts, with the lattice supporting coating growth and enabling recovery and reuse as a single structure.
Related
- SnFe2O4–rGO heterojunction for visible light driven photocatalytic degradation of methylene blue: a combined experimental and theoretical study
- Unveiling the photocatalytic degradation mechanism of methylene blue on the octahedral Cu2O(111) facets
- Valorization of Industrial Mill Scales into Multiphase Iron Oxide Nanostructures for Alkaline Water Splitting and Photocatalytic Dye Degradation
- Plasmonic Ag@ZIF-8 Monolith for Enhanced Visible-Light Photocatalytic Degradation of Methylene Blue
- Photocatalytic performance and surface characterization of plant-mediated ZnO nanoparticles for methylene blue degradation
BibTeX
@article{yavas2026cumodified,
title = {{Cu-modified ZnO nanostructures on 3D-printed photopolymer scaffolds for reusable photocatalytic degradation of methylene blue}},
author = {Ahmet Yavaş},
journal = {RSC advances},
year = {2026},
month = nov,
doi = {10.1039/d6ra09099k},
url = {https://europepmc.org/article/PMC/PMC13787356},
note = {CC BY},
}
RIS
TY - JOUR
TI - Cu-modified ZnO nanostructures on 3D-printed photopolymer scaffolds for reusable photocatalytic degradation of methylene blue
AU - Ahmet Yavaş
PY - 2026
DA - 2026/11/20
JO - RSC advances
DO - 10.1039/d6ra09099k
UR - https://europepmc.org/article/PMC/PMC13787356
AB - Cu-modified ZnO nanostructures were hydrothermally grown on three-dimensional epoxy/acrylate photopolymer scaffolds fabricated by LCD-based vat photopolymerization. After surface activation and ZnO seed-layer deposition, coatings with nominal Cu contents of 0.5, 1, and 2 wt% were grown at 90 °C for 4 h. X-ray diffraction and Raman spectroscopy confirmed preservation of hexagonal wurtzite ZnO, while Cu addition modified the principal diffraction reflections without detectable secondary Cu-containing crystalline phases. Electron microscopy and elemental analysis revealed dense rod-like nanostructures with Cu-dependent morphology and verified Cu in the coatings. Optical measurements showed Cu-dependent changes in reflectance, band-gap energy, and defect-related emission. After 180 min under artificial sunlight, the mean methylene blue (MB) degradation efficiency increased from (54.59 ± 1.61)% for ZnO/P to (83.67 ± 1.08)% for 2Cu–ZnO/P. The latter exhibited an apparent rate constant of (8.78 ± 0.39) × 10−3 min−1, approximately 2.2 times that of ZnO/P. Scavenger experiments indicated a predominant role of superoxide radicals under the investigated conditions. One of the three 2Cu–ZnO/P scaffolds was used for four additional cycles. Its MB degradation efficiency decreased from 84.88% in cycle 1 to 78.11% in cycle 5, corresponding to 92.02% retention of its first-cycle efficiency. These results demonstrate the potential of Cu-modified ZnO on open cubic vertex-centroid scaffolds as reusable immobilized photocatalysts, with the lattice supporting coating growth and enabling recovery and reuse as a single structure.
SN - 2046-2069
ER -