An Ultrathin Laterally Conductive Mesh Interphase Enables Spatially Extended Zinc Deposition for Aqueous Zinc Batteries
Abstract
Zn metal anodes often suffer from nonuniform interfacial reactions during cycling, resulting in uneven deposition and dendrite growth. Existing artificial interphases can mitigate side reactions or regulate nucleation, but rarely achieve regulation of the interfacial electron/field distribution to sustain uniform deposition at the evolving Zn/electrolyte interface. Here, we develop an Au mesh interphase (AuMI), an ultrathin two-dimensional Au aerogel network that couples lateral electron redistribution with open pathways for ions. During Zn plating/stripping, the conductive AuMI distributes electron transport across the Zn surface, while its porous mesh preserves Zn2+ access, enabling more uniform interfacial reactions. Experiments and simulations show that AuMI homogenizes the interfacial electric field and current distribution, promotes more uniform Zn plating/stripping, and limits dendrite growth. As a result, this regulated interfacial reaction mode enables AuMI Zn symmetric cells to operate stably for 3000 h at 1 mA cm−2/1 mAh cm−2 and for 1100 h at 10 mA cm−2/10 mAh cm−2, while AuMI Zn||NVO (NaV3O8\cdot1.5H_2$O) full cells retain 80.8 % capacity after over 5000 cycles at 1 A g−1. These findings highlight the importance of combining ultrathin architecture, lateral electron transport, and open Zn2+ access in artificial interphases for stable aqueous Zn metal anodes.
Related
- The quantized Hall effect knows which way the current flows: mirror covariance and rectification in a laterally asymmetric Hall bar
- Streamwise dispersion with interphase mass transfer through a tube
- Intercalation of Ultrathin Ferromagnetic Iron Films at the Graphene/SiC Interface
- Selective Operando Visualization of Ultrathin Lithium in Li-Metal Batteries by Neutron Capture Imaging
- Deterministic and dynamic synthesis of optical skyrmions through an ultrathin multimode fibre
BibTeX
@misc{zhao2026ultrathin,
title = {{An Ultrathin Laterally Conductive Mesh Interphase Enables Spatially Extended Zinc Deposition for Aqueous Zinc Batteries}},
author = {Yirong Zhao and Xingyuan Chu and Bing Wu and Pavel Khavlyuk and Johannes Kresse and Yue Dong and Jingwei Du and Xinmei Song and Songshan Bi and Vlastimil Mazanek and Xia Wang and Xiaodong Li and Shilei Liu and Shuangying Wei and Jan Luxa and Junming Zhang and Zdenek Sofer and Alexander Eychmuller},
howpublished = {arXiv},
year = {2026},
month = sep,
doi = {10.48550/arxiv.2609.03176},
eprint = {2609.03176},
archivePrefix = {arXiv},
url = {https://arxiv.org/abs/2609.03176},
}
RIS
TY - UNPB
TI - An Ultrathin Laterally Conductive Mesh Interphase Enables Spatially Extended Zinc Deposition for Aqueous Zinc Batteries
AU - Yirong Zhao
AU - Xingyuan Chu
AU - Bing Wu
AU - Pavel Khavlyuk
AU - Johannes Kresse
AU - Yue Dong
AU - Jingwei Du
AU - Xinmei Song
AU - Songshan Bi
AU - Vlastimil Mazanek
AU - Xia Wang
AU - Xiaodong Li
AU - Shilei Liu
AU - Shuangying Wei
AU - Jan Luxa
AU - Junming Zhang
AU - Zdenek Sofer
AU - Alexander Eychmuller
PY - 2026
DA - 2026/09/02
PB - arXiv
DO - 10.48550/arxiv.2609.03176
UR - https://arxiv.org/abs/2609.03176
AB - Zn metal anodes often suffer from nonuniform interfacial reactions during cycling, resulting in uneven deposition and dendrite growth. Existing artificial interphases can mitigate side reactions or regulate nucleation, but rarely achieve regulation of the interfacial electron/field distribution to sustain uniform deposition at the evolving Zn/electrolyte interface. Here, we develop an Au mesh interphase (AuMI), an ultrathin two-dimensional Au aerogel network that couples lateral electron redistribution with open pathways for ions. During Zn plating/stripping, the conductive AuMI distributes electron transport across the Zn surface, while its porous mesh preserves Zn^2+ access, enabling more uniform interfacial reactions. Experiments and simulations show that AuMI homogenizes the interfacial electric field and current distribution, promotes more uniform Zn plating/stripping, and limits dendrite growth. As a result, this regulated interfacial reaction mode enables AuMI Zn symmetric cells to operate stably for 3000 h at 1 mA cm^−2/1 mAh cm^−2 and for 1100 h at 10 mA cm^−2/10 mAh cm^−2, while AuMI Zn||NVO (NaV_3O_8\cdot1.5H_2$O) full cells retain 80.8 % capacity after over 5000 cycles at 1 A g^−1. These findings highlight the importance of combining ultrathin architecture, lateral electron transport, and open Zn2+ access in artificial interphases for stable aqueous Zn metal anodes.