Skip to content
DraconiticResearch
Search Sources API
203,234 studies31 sourcesUpdated 52 min ago
PreprintarXiv licencearXiv

A colossal dielectric response of Bi1-xSmxFeO3 nanopowders

Abstract

The dielectric permittivity of the pressed powder samples of Bi1-xSmxFeO3, with Sm content "x" varying in the range 0 - 0.2, has been investigated in the temperature range from 20 to 400 C and the frequency range from 100 Hz to 100 kHz. We have shown that the Sm content impacts significantly the real and imaginary parts of effective dielectric permittivity, which have expanded diffuse maxima with a colossal magnitude up to 105 (for the real part) and up to 108 (for the imaginary one) at temperatures 300 - 400 K. Analysis of experimental data carried has shown that both the real and imaginary parts of effective dielectric permittivity may be comprehensively explained by considering a complex interplay of a diffuse ferroelectric-paraelectric phase transition and the Maxwell-Wagner-Sillars effects, which emerge from the formation of spatial charges at interfaces between nanograins and at the ferroelectric nanoparticle-air interface. Processing of experimental data for the real and imaginary parts of the effective dielectric permittivity within effective medium approach allows us to separate and analyze the colossal dielectric response of the nanoparticles itself. The main trends followed from experiments are supported by the theoretically simulated dependences, which reveal correlations between the temperature behavior of dielectric properties and phase state of the Bi1-xSmxFeO3 nanoparticles.

Related

  1. Angular compliance, not amplitude, governs the dielectric response of BaTiO3
    Ryotaro Sahashi, Po-Yen Chen, Teruyasu Mizoguchi
    arXivPreprintCC BY 4.0Full textCondensed matterarXiv
  2. A Mean-Field Approach to the Dielectric Response of Bulk Superconductors for Light Dark Matter Direct Detection
    Chengyao Gan, Hui Li, Wenjing Li +3
    arXivPreprintCC BY 4.0Full textHigh-energy & particle physicsarXiv
  3. Dielectric response of the antiferromagnetic multiferroics with cycloidal equilibrium for the polarization related to the noncollinear spins
    Pavel A. Andreev
    arXivPreprintCC BY 4.0Full textCondensed matterarXiv
  4. Atom-Resolved Machine Learning of Dielectric and Piezoelectric Response
    Jinyu Liu, Yingwei Chen, Liyang Ma +2
    arXivPreprintarXiv licenceFull textCondensed matterarXiv
  5. First-Principles Prediction of Nonlinear Optical Response in TiO2 for High-Power Dielectric Mirror Applications
    Koya Shimaoka, Yusuke Kondo, Kazunori Shibata +1
    arXivPreprintarXiv licenceFull textCondensed matterOptics & photonicsarXiv
BibTeX
@misc{kolupaiev2026colossal,
  title = {{A colossal dielectric response of Bi1-xSmxFeO3 nanopowders}},
  author = {Vladyslav O. Kolupaiev and Olexander S. Pylypchuk and Vladimir N. Poroshin and Denis O. Stetsenko and Ihor V. Fesych and Lesya D. Demchenko and Eugene A. Eliseev and Victor V. Vainberg and Anna N. Morozovska},
  howpublished = {arXiv},
  year = {2026},
  month = sep,
  doi = {10.48550/arxiv.2608.24420},
  eprint = {2608.24420},
  archivePrefix = {arXiv},
  url = {https://arxiv.org/abs/2608.24420},
}
RIS
TY  - UNPB
TI  - A colossal dielectric response of Bi1-xSmxFeO3 nanopowders
AU  - Vladyslav O. Kolupaiev
AU  - Olexander S. Pylypchuk
AU  - Vladimir N. Poroshin
AU  - Denis O. Stetsenko
AU  - Ihor V. Fesych
AU  - Lesya D. Demchenko
AU  - Eugene A. Eliseev
AU  - Victor V. Vainberg
AU  - Anna N. Morozovska
PY  - 2026
DA  - 2026/09/14
PB  - arXiv
DO  - 10.48550/arxiv.2608.24420
UR  - https://arxiv.org/abs/2608.24420
AB  - The dielectric permittivity of the pressed powder samples of Bi1-xSmxFeO3, with Sm content "x" varying in the range 0 - 0.2, has been investigated in the temperature range from 20 to 400 C and the frequency range from 100 Hz to 100 kHz. We have shown that the Sm content impacts significantly the real and imaginary parts of effective dielectric permittivity, which have expanded diffuse maxima with a colossal magnitude up to 105 (for the real part) and up to 108 (for the imaginary one) at temperatures 300 - 400 K. Analysis of experimental data carried has shown that both the real and imaginary parts of effective dielectric permittivity may be comprehensively explained by considering a complex interplay of a diffuse ferroelectric-paraelectric phase transition and the Maxwell-Wagner-Sillars effects, which emerge from the formation of spatial charges at interfaces between nanograins and at the ferroelectric nanoparticle-air interface. Processing of experimental data for the real and imaginary parts of the effective dielectric permittivity within effective medium approach allows us to separate and analyze the colossal dielectric response of the nanoparticles itself. The main trends followed from experiments are supported by the theoretically simulated dependences, which reveal correlations between the temperature behavior of dielectric properties and phase state of the Bi1-xSmxFeO3 nanoparticles.