Skip to content
DraconiticResearch
Search Sources API
277,308 studies31 sourcesUpdated 54 min ago
Peer-reviewedCC BY 4.0Catalysts

Deciphering Local Structure Restructuring in Phosphate-Modified Nanocrystalline ZSM-5 Under Hydrothermal Conditions

  1. 1School of Materials, Sun Yat-sen University, Shenzhen 518107, China
  2. 2Lanzhou Petrochemical Research Center, Petrochemical Research Institute, PetroChina, Lanzhou 730060, China

Abstract

Nanocrystalline H-ZSM-5 zeolites effectively shorten intracrystalline diffusion paths and suppress coking; however, their elevated interfacial surface energy renders them exceptionally vulnerable to severe hydrothermal dealumination. Herein, we employ multinuclear solid-state NMR (27Al, 31P HPDEC/MAS, and 1H-31P CP/MAS), XRD, and N2 physisorption to decipher the local structural transformations in phosphate-modified nano-ZSM-5 (2–10 wt% P2O5) before and after severe hydrothermal aging (800 °C, 100% steam). In unsteamed samples, phosphorus resides largely as weakly bound, mobile precursors lacking direct framework coordination. Severe steaming acts as an in situ structural reorganizer; it strips labile surface species while driving reactive precursors to form chemically anchored, hydroxylated Al-O-P linkages (centered at −29.4 ppm in 31P NMR). These anchors perturb tetrahedral framework aluminum, shifting it into distorted environments and effectively suppressing hydrolytic dealumination. Beyond framework aluminum saturation, excess phosphorus condenses into non-hydroxylated, cage-like P4O10 clusters (−38.3 ppm in 31P NMR). Textural evaluations confirm that moderate loading (2 wt% P2O5) preserves specific surface area (309.4 m2 g−1) and microporosity, whereas higher loadings (≥4 wt% P2O5) incur progressive micropore constriction in exchange for sacrificial buffering against steam-induced degradation. These findings provide fundamental structural insights into mitigating hydrothermal degradation in nanoscale zeolite frameworks.

Related

  1. Chemical Filtering of Thymine over Uracil by Differential Hydrolysis under Dark Alkaline Hydrothermal-Vent Conditions: A Mass-Consistent, Control-Restrained Simulation Framework (UPDSF v6.7.0)
    Seyed Mohammad Reza Hashemi
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  2. Hydrothermal Zn–Fe Mixed Oxide Nanocatalysts: Influence of Synthesis Conditions on Physicochemical Properties, Acidity, and Catalytic Activity in the Biginelli Reaction
    Samira Slyemi, Juliette Blanchard, Ouzna Kheffache +5
    Chemistry AfricaPeer-reviewedCC BY-NC 4.0Full textCatalysisMaterials & polymersHAL
  3. Deciphering Ionic Conductivity Differences in Linear Carbonate Electrolytes: Conformational Shrinkage and Solvation Structure in Dimethyl vs Diethyl Carbonate
    Mansi Jain, Sundaram Balasubramanian
    ChemRxivPreprintCC BYFull textGeneral chemistryChemRxiv
  4. Synthesis of Nanocrystalline Gd2O2NCN from a Versatile Single-source Precursor
    Emanuel Ionescu, Wenjie Li, Leonore Wiehl +2
    Zeitschrift fur Anorganische und Allgemeine ChemiePeer-reviewedLicence not statedFull text5 citedInorganic & organometallic chemistryHAL
  5. Sustainable production of pure nanocrystalline cellulose (NCCs) as a binder for enhanced aspirin tablets: Valorization of palm kernel waste
    Fahd M. Alminderej, Wael A. El-Sayed, Tamer I. M. Ragab
    Scientific ReportsPeer-reviewedCC BY-NC-ND 4.0Full textMaterials & polymersCrossref
BibTeX
@article{tang2026deciphering,
  title = {{Deciphering Local Structure Restructuring in Phosphate-Modified Nanocrystalline ZSM-5 Under Hydrothermal Conditions}},
  author = {Wei Tang and Mengyuan Fan and Jiejun Yao and Xiaohui Du and Xiaolong Liu},
  journal = {Catalysts},
  year = {2026},
  month = nov,
  doi = {10.3390/catal16111023},
  url = {https://www.mdpi.com/2073-4344/16/11/1023},
  note = {CC BY 4.0},
}
RIS
TY  - JOUR
TI  - Deciphering Local Structure Restructuring in Phosphate-Modified Nanocrystalline ZSM-5 Under Hydrothermal Conditions
AU  - Wei Tang
AU  - Mengyuan Fan
AU  - Jiejun Yao
AU  - Xiaohui Du
AU  - Xiaolong Liu
PY  - 2026
DA  - 2026/11/17
JO  - Catalysts
DO  - 10.3390/catal16111023
UR  - https://www.mdpi.com/2073-4344/16/11/1023
AB  - Nanocrystalline H-ZSM-5 zeolites effectively shorten intracrystalline diffusion paths and suppress coking; however, their elevated interfacial surface energy renders them exceptionally vulnerable to severe hydrothermal dealumination. Herein, we employ multinuclear solid-state NMR (27Al, 31P HPDEC/MAS, and 1H-31P CP/MAS), XRD, and N2 physisorption to decipher the local structural transformations in phosphate-modified nano-ZSM-5 (2–10 wt% P2O5) before and after severe hydrothermal aging (800 °C, 100% steam). In unsteamed samples, phosphorus resides largely as weakly bound, mobile precursors lacking direct framework coordination. Severe steaming acts as an in situ structural reorganizer; it strips labile surface species while driving reactive precursors to form chemically anchored, hydroxylated Al-O-P linkages (centered at −29.4 ppm in 31P NMR). These anchors perturb tetrahedral framework aluminum, shifting it into distorted environments and effectively suppressing hydrolytic dealumination. Beyond framework aluminum saturation, excess phosphorus condenses into non-hydroxylated, cage-like P4O10 clusters (−38.3 ppm in 31P NMR). Textural evaluations confirm that moderate loading (2 wt% P2O5) preserves specific surface area (309.4 m2 g−1) and microporosity, whereas higher loadings (≥4 wt% P2O5) incur progressive micropore constriction in exchange for sacrificial buffering against steam-induced degradation. These findings provide fundamental structural insights into mitigating hydrothermal degradation in nanoscale zeolite frameworks.
SN  - 2073-4344
ER  -