Feasibility of 3D-printed polylactic acid (PLA) osteosynthesis plates: an ex vivo biomechanical study.

5 affiliations
  1. 1Marburg University, Marburg, Germany. [email protected].
  2. 2Center for Orthopaedics and Trauma Surgery, University Hospital Gießen and Marburg, Marburg, Germany. [email protected].
  3. 3Marburg University, Marburg, Germany.
  4. 4Department of Physics, Marburg University, Marburg, Germany.
  5. 5Center for Orthopaedics and Trauma Surgery, University Hospital Gießen and Marburg, Marburg, Germany.

Abstract

Metallic osteosynthesis plates provide excellent stability but frequently require secondary removal surgeries. Bioresorbable 3D-printed polylactic acid (PLA) could be an alternative. This study aimed to evaluate mechanical feasibility of 3D-printed PLA plates in an ex vivo model - under static/cyclic loading and assess hydrolytic degradation over 12 months. Porcine metatarsals with standardized AO/OTA A2 fractures were stabilized using 2.0 mm Dynamic Compression Plates (DCP®, Synthes®) or Fused Deposition Modelling (FDM)-manufactured PLA plate prototypes (100% and 20% infill density). Isolated PLA plates and osteosynthesis constructs underwent three-point bending tests. The biomechanical performance of the PLA plates was evaluated after hydrolytic degradation in phosphate-buffered saline. The statistical analysis was performed using ANOVA or Kruskal-Wallis tests with Bonferroni post hoc correction (p < 0.05). Isolated PLA plates failed at 61-74 N confirming insufficient standalone stability. Osteosynthesis constructs, however, achieved comparable maximum load (p = 0.087) and stiffness (p = 0.104) to metal controls under static loading, with failure primarily via plate fracture (vs. screw pull-out in metal). Cyclic testing revealed significantly earlier failures (p = 0.004 / 0.014). Hydrolysed plates (12 months) showed reduced maximum load (p < 0.001), deformation (p < 0.05), and stiffness (p < 0.01), with stability maintained through week 6. Considering ex vivo study limitations, PLA plates demonstrate initial construct stability under static loading and predictable hydrolytic degradation, while exhibiting reduced fatigue resistance. Clinical applicability is not yet established. The 20% infill architecture may provide internal reservoirs for drug delivery in future investigations. This graphic explains the process and testing of 3D printed bioresorbable plates made from PLA material. It shows that plates are printed with either 100 percent infill or 20 percent infill containing tri-hexagonal reservoirs. Three tests are performed on the plates: maximum load, cyclic testing, and hydrolysis up to 12 months. Results indicate that metal plates have higher maximum load and cyclic testing values than PLA plates. Over 12 months of hydrolysis, the maximum load of PLA plates decreases. Future investigations include using finite element analysis to improve cyclic loading, creating drug-loaded PLA plates, studying drug release through hydrolysis, and conducting in vivo analysis in animals.

Related

  1. Feasibility of Intraoperative Anterior Reduction for the Treatment of Grade II Spondylolisthesis: A Biomechanical Investigation
    Deepak Reddy, Joshua P. McGuckin, Derek Yocum +4
    International Journal of Spine SurgeryPeer-reviewedLicence not statedFull textSurgery & anaesthesiaPMC
  2. Feasibility of patient-specific 3D-printed fragment models for preoperative planning in bicondylar tibial plateau fractures: a retrospective case series
    Lixiong Cai, Zhiling Liao, Weibing Liu +3
    Frontiers in MedicinePeer-reviewedCC BY 4.0Full textSurgery & anaesthesiaPMCEurope PMC
  3. Unburied Versus Buried Kirschner Wires in the Traumatic Osteosynthesis of the Upper Limb in Pediatric Patients: A Retrospective Cohort
    Journal of the American Academy of Orthopaedic Surgeons. Global research & reviewsPeer-reviewedCC BY-NC-NDFull textSurgery & anaesthesiaEurope PMC
  4. Hybrid Osteosynthesis for Septic Humeral Shaft Nonunion in a Patient with Obesity: A Case Report.
    Paolo Chiquini-Ramírez, Nancy Lorena Villamues-Moreno, Jorge Ponce-de-Léon-Dominguez +5
    CureusPeer-reviewedCC BYFull textInfectious diseaseEurope PMCPMC
  5. Functional Outcomes of Midshaft Clavicle Fractures Treated With Plate Osteosynthesis: A Prospective Observational Study
    Brijendra Singh, Rohit Shukla, Shubham Srivastava +2
    CureusPeer-reviewedCC BYFull textEpidemiology & public healthEurope PMCPMC
BibTeX
@article{santos2026feasibility,
  title = {{Feasibility of 3D-printed polylactic acid (PLA) osteosynthesis plates: an ex vivo biomechanical study.}},
  author = {Vanessa Dos Santos and Jan Helminiak and Jakob Cornelius and Muriel Canarius and Martin Koch and Steffen Ruchholtz and Jürgen R J Paletta and Martin Bäumlein},
  journal = {Journal of materials science. Materials in medicine},
  year = {2026},
  month = nov,
  doi = {10.1007/s10856-026-07138-8},
  url = {https://europepmc.org/article/MED/43077145},
  note = {CC BY},
}
RIS
TY  - JOUR
TI  - Feasibility of 3D-printed polylactic acid (PLA) osteosynthesis plates: an ex vivo biomechanical study.
AU  - Vanessa Dos Santos
AU  - Jan Helminiak
AU  - Jakob Cornelius
AU  - Muriel Canarius
AU  - Martin Koch
AU  - Steffen Ruchholtz
AU  - Jürgen R J Paletta
AU  - Martin Bäumlein
PY  - 2026
DA  - 2026/11/24
JO  - Journal of materials science. Materials in medicine
DO  - 10.1007/s10856-026-07138-8
UR  - https://europepmc.org/article/MED/43077145
AB  - Metallic osteosynthesis plates provide excellent stability but frequently require secondary removal surgeries. Bioresorbable 3D-printed polylactic acid (PLA) could be an alternative. This study aimed to evaluate mechanical feasibility of 3D-printed PLA plates in an ex vivo model - under static/cyclic loading and assess hydrolytic degradation over 12 months. Porcine metatarsals with standardized AO/OTA A2 fractures were stabilized using 2.0 mm Dynamic Compression Plates (DCP®, Synthes®) or Fused Deposition Modelling (FDM)-manufactured PLA plate prototypes (100% and 20% infill density). Isolated PLA plates and osteosynthesis constructs underwent three-point bending tests. The biomechanical performance of the PLA plates was evaluated after hydrolytic degradation in phosphate-buffered saline. The statistical analysis was performed using ANOVA or Kruskal-Wallis tests with Bonferroni post hoc correction (p < 0.05). Isolated PLA plates failed at 61-74 N confirming insufficient standalone stability. Osteosynthesis constructs, however, achieved comparable maximum load (p = 0.087) and stiffness (p = 0.104) to metal controls under static loading, with failure primarily via plate fracture (vs. screw pull-out in metal). Cyclic testing revealed significantly earlier failures (p = 0.004 / 0.014). Hydrolysed plates (12 months) showed reduced maximum load (p < 0.001), deformation (p < 0.05), and stiffness (p < 0.01), with stability maintained through week 6. Considering ex vivo study limitations, PLA plates demonstrate initial construct stability under static loading and predictable hydrolytic degradation, while exhibiting reduced fatigue resistance. Clinical applicability is not yet established. The 20% infill architecture may provide internal reservoirs for drug delivery in future investigations. This graphic explains the process and testing of 3D printed bioresorbable plates made from PLA material. It shows that plates are printed with either 100 percent infill or 20 percent infill containing tri-hexagonal reservoirs. Three tests are performed on the plates: maximum load, cyclic testing, and hydrolysis up to 12 months. Results indicate that metal plates have higher maximum load and cyclic testing values than PLA plates. Over 12 months of hydrolysis, the maximum load of PLA plates decreases. Future investigations include using finite element analysis to improve cyclic loading, creating drug-loaded PLA plates, studying drug release through hydrolysis, and conducting in vivo analysis in animals.
SN  - 0957-4530
SN  - 1573-4838
ER  -