Abstract

In‐situ gel polymer electrolytes (GPEs) have attracted attention as promising candidates for next‐generation lithium‐ion batteries, offering superior interfacial compatibility and enhanced safety compared with conventional liquid electrolytes. However, the issue of residual monomers remaining after polymerization has not been adequately addressed. They readily decompose at the high‐Ni cathode (NCM) surface during the early stage of formation, generating an organic‐rich layer within the inner cathode–electrolyte interphase (CEI) and disrupting the normal CEI‐forming pathway. Here, we present a strategy that combines a molecular additive, tris(4‐fluorophenyl)phosphine (TFPP), with a tailored formation protocol to mitigate monomer‐induced degradation. Prior to oxidative decomposition, TFPP modifies the interfacial environment of NCM through early surface interaction and partial coverage, reducing the accessibility of residual monomers to the cathode interface. The formation protocol then promotes preferential TFPP decomposition before extensive monomer oxidation, enabling a protective CEI with a LiF‐rich inner region. This sequential interfacial regulation suppresses monomer‐driven side reactions, reduces electrolyte consumption, stabilizes Li‐ion transport, and mitigates structural degradation of the cathode. Consequently, a 2 Ah‐level pouch cell delivering 303 Wh kg−1 retained 82.8% capacity after 150 cycles under lean electrolyte conditions (2 g Ah−1). This work thus provides a practical strategy for developing more durable high‐energy‐density GPE‐based batteries.

Related

  1. Computational Modeling of Electrolytes and the Solid–Electrolyte Interphase (SEI) in Li-Ion Batteries: A 30-Year Odyssey from DFT/MD/MC to AI–A Comprehensive Review
    Ilya V. Chepkasov, Alexey S. Galushko, Viktor S. Baidyshev +3
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  2. Stable lithium/electrolyte interphase enabled by tailoring Li+ solvation structure and FEC additive in LiOTf/LiNO3 dual-salt sulfolane-based nonflammable electrolyte for lithium metal batteries
    Chun-Jern Pan, Yi-Yu Chen, Jia-He Peng +2
    Electrochemistry CommunicationsPeer-reviewedCC BY-NC 4.0Full textElectrochemistry & energyCrossrefDOAJ
  3. Ionic liquid electrolytes for graphite in potassium-ion batteries: the effect of anions on solid-electrolyte interphase.
    Tianyi Shi, Avishek Dey, Yuhan Liu +4
    Journal of materials chemistry. APeer-reviewedCC BYFull textGeneral chemistryEurope PMCPMC
  4. Complementary anion chemistry enabling coordination pre-organization towards a robust disordered interphase for long-life aqueous Zn batteries
    Xiaoxin Nie, Yujiao Yang, Xin Liu +4
    Chemical sciencePeer-reviewedCC BY-NCFull textOrganic chemistryEurope PMC
  5. Symmetric dual-interphase design enables stable lithium-metal anodes for high rate ultrahigh-nickel all-solid-state batteries
    Chen Liu, Zhuolin Zhong, Lin Li +6
    Chemical sciencePeer-reviewedCC BY-NCFull textOrganic chemistryEurope PMC
BibTeX
@article{kang2026mechanistic,
  title = {{Mechanistic Control of Cathode–Electrolyte Interphase Formation in Gel Polymer Electrolyte for Lithium‐Ion Batteries}},
  author = {Sang Goo Kang and Jeonghyun Ko and Gunyoung Kim and Jaehoon Choi and Jong Hyeok Park},
  journal = {Angewandte Chemie (International Ed. in English)},
  year = {2026},
  month = sep,
  doi = {10.1002/anie.1297472},
  url = {https://doi.org/10.1002/anie.1297472},
  note = {CC BY-NC 4.0},
}
RIS
TY  - JOUR
TI  - Mechanistic Control of Cathode–Electrolyte Interphase Formation in Gel Polymer Electrolyte for Lithium‐Ion Batteries
AU  - Sang Goo Kang
AU  - Jeonghyun Ko
AU  - Gunyoung Kim
AU  - Jaehoon Choi
AU  - Jong Hyeok Park
PY  - 2026
DA  - 2026/09/28
JO  - Angewandte Chemie (International Ed. in English)
DO  - 10.1002/anie.1297472
UR  - https://doi.org/10.1002/anie.1297472
AB  - In‐situ gel polymer electrolytes (GPEs) have attracted attention as promising candidates for next‐generation lithium‐ion batteries, offering superior interfacial compatibility and enhanced safety compared with conventional liquid electrolytes. However, the issue of residual monomers remaining after polymerization has not been adequately addressed. They readily decompose at the high‐Ni cathode (NCM) surface during the early stage of formation, generating an organic‐rich layer within the inner cathode–electrolyte interphase (CEI) and disrupting the normal CEI‐forming pathway. Here, we present a strategy that combines a molecular additive, tris(4‐fluorophenyl)phosphine (TFPP), with a tailored formation protocol to mitigate monomer‐induced degradation. Prior to oxidative decomposition, TFPP modifies the interfacial environment of NCM through early surface interaction and partial coverage, reducing the accessibility of residual monomers to the cathode interface. The formation protocol then promotes preferential TFPP decomposition before extensive monomer oxidation, enabling a protective CEI with a LiF‐rich inner region. This sequential interfacial regulation suppresses monomer‐driven side reactions, reduces electrolyte consumption, stabilizes Li‐ion transport, and mitigates structural degradation of the cathode. Consequently, a 2 Ah‐level pouch cell delivering 303 Wh kg−1 retained 82.8% capacity after 150 cycles under lean electrolyte conditions (2 g Ah−1). This work thus provides a practical strategy for developing more durable high‐energy‐density GPE‐based batteries.
SN  - 1433-7851
SN  - 1521-3773
ER  -