Synergistic Stabilization of Aeolian Sand Using Phosphogypsum-Based Materials: Mechanical Performance and Microstructural Evolution
- 1China Construction Institute of Advanced Technology, Wuhan 430073, China
- 2Faculty of Engineering, China University of Geosciences, Wuhan 430074, China
Abstract
Large-scale desert ecological restoration is constrained by three coupled problems: aeolian sand aggregates poorly and cannot sustain vegetation; stockpiled phosphogypsum imposes a persistent environmental burden; and importing and ameliorating exogenous topsoil is costly. This study evaluated wet-ground modified phosphogypsum (PG-A), as-received phosphogypsum used as aggregate (PG-B), aeolian sand (AS), and phosphogypsum-based supersulfated cement (PPSC). The liquid–plastic limit, compaction, direct-shear, unconfined compressive strength (UCS), and leaching tests were performed. The plasticity index of the PG-B-AS mixtures ranged from 6.62 to 12.31, and the maximum dry density increased with the AS fraction and with the PPSC content under the tested conditions. For PG-B:AS mass ratios from 1:3 to 3:1, the leachate pH ranged from 6.79 to 7.79. When AS constituted at least 25% of the aggregate, soluble phosphorus met the Class V limit of GB 3838-2002, fluoride met the Class I limit, and the phosphorus stabilization efficiency exceeded 93.5%, reaching 96.9% for GL-16 (PG-B:AS = 25:75, 15% PPSC). Room-temperature 14- and 28-day UCS values ranged from 0.602 to 1.950 MPa and from 0.853 to 2.250 MPa, respectively. The mechanical performance improved with a higher PG-B fraction, whereas the environmental fixation improved in the opposite direction. The XRD and SEM revealed quartz, gypsum, ettringite, and C-S-H development during curing. Within the tested range, PG-B:AS = 25:75 with 12–15% PPSC provided the clearest balance between leachate compliance and retained mechanical improvement.
Related
- Cell-free reconstitution reveals synergistic stabilization of microtubule doublets by PACRG and FAP20
- Enhancing physiological performance and antioxidant defense in Mexican lime (Citrus aurantifolia) under water-deficit: synergistic effects of PGPB and KNO₃ application
- Possible Mechanical Stabilization of the Photoreceptor Connecting Cilium: From Molecular Scaffolds to Drug Repurposing
- Closed-loop cognitive state control: a hypothesis framework for real-time estimation, stabilization, and recovery of task-specific high-performance cognitive states.
- Upcycling Recycled PET into High-Performance Polyurethane Coating and Engineering Materials: Effect of NCO Index on Mechanical, Stability, and Surface Properties
BibTeX
@article{jia2026synergistic,
title = {{Synergistic Stabilization of Aeolian Sand Using Phosphogypsum-Based Materials: Mechanical Performance and Microstructural Evolution}},
author = {Ruihua Jia and Junfeng Hu and Zeyi Bie and Rui Li and Heyu Wang and Changwei Zhang and Fang Xu},
journal = {Applied Sciences},
year = {2026},
month = nov,
doi = {10.3390/app162111076},
url = {https://doi.org/10.3390/app162111076},
note = {CC BY},
}
RIS
TY - JOUR
TI - Synergistic Stabilization of Aeolian Sand Using Phosphogypsum-Based Materials: Mechanical Performance and Microstructural Evolution
AU - Ruihua Jia
AU - Junfeng Hu
AU - Zeyi Bie
AU - Rui Li
AU - Heyu Wang
AU - Changwei Zhang
AU - Fang Xu
PY - 2026
DA - 2026/11/13
JO - Applied Sciences
DO - 10.3390/app162111076
UR - https://doi.org/10.3390/app162111076
AB - Large-scale desert ecological restoration is constrained by three coupled problems: aeolian sand aggregates poorly and cannot sustain vegetation; stockpiled phosphogypsum imposes a persistent environmental burden; and importing and ameliorating exogenous topsoil is costly. This study evaluated wet-ground modified phosphogypsum (PG-A), as-received phosphogypsum used as aggregate (PG-B), aeolian sand (AS), and phosphogypsum-based supersulfated cement (PPSC). The liquid–plastic limit, compaction, direct-shear, unconfined compressive strength (UCS), and leaching tests were performed. The plasticity index of the PG-B-AS mixtures ranged from 6.62 to 12.31, and the maximum dry density increased with the AS fraction and with the PPSC content under the tested conditions. For PG-B:AS mass ratios from 1:3 to 3:1, the leachate pH ranged from 6.79 to 7.79. When AS constituted at least 25% of the aggregate, soluble phosphorus met the Class V limit of GB 3838-2002, fluoride met the Class I limit, and the phosphorus stabilization efficiency exceeded 93.5%, reaching 96.9% for GL-16 (PG-B:AS = 25:75, 15% PPSC). Room-temperature 14- and 28-day UCS values ranged from 0.602 to 1.950 MPa and from 0.853 to 2.250 MPa, respectively. The mechanical performance improved with a higher PG-B fraction, whereas the environmental fixation improved in the opposite direction. The XRD and SEM revealed quartz, gypsum, ettringite, and C-S-H development during curing. Within the tested range, PG-B:AS = 25:75 with 12–15% PPSC provided the clearest balance between leachate compliance and retained mechanical improvement.
SN - 2076-3417
ER -