Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers
- 1School of Materials Science and Engineering, PCFM Lab, Key Laboratory of Low-Carbon Chemistry and Energy Conservation of Guangdong Province, Sun Yat-sen University, Guangzhou 510275, China
Abstract
Poly(propylene carbonate) diol (PPCDL) can incorporate CO2 directly into the soft segment of a thermoplastic polyurethane (TPU); however, its rigid and strongly polar carbonate backbone suppresses microphase separation, so lower hardness is usually achieved only at the expense of tensile strength. Herein, this trade-off was addressed by molecular design rather than formulation adjustment within this fixed formulation window. By utilizing a rigid–flexible synergetic strategy, six heterocyclic siloxane modifiers bearing triazole, thiadiazole, or aniline pendants, along with three amino-terminated poly(dimethylsiloxane) (PDMS) controls, were incorporated into PPCDL-based TPUs as chain-extending segments via a torque-rheometer-assisted bulk process at a fixed hard-segment content of 17 wt% and a [NCO]/[OH] ratio of 1.02. Each modifier couples a flexible siloxane spacer with heterocyclic hydrogen-bonding moieties, and the N–H donor and sp2-hybridized nitrogen acceptor counts were explicitly enumerated. The long-chain triazole modifier L2 afforded the most balanced elastomer, with a Shore A hardness of 76, a tensile strength of 5.71 ± 0.44 MPa, and an elongation at break of 892 ± 54%; these values exceeded those of the best PDMS control (4.36 ± 0.33 MPa, 621 ± 0.97%, 80 Shore A) in all evaluated metrics, without any petroleum-based polyol. Gaussian deconvolution of the N–H stretching band showed that the ordered hydrogen-bonded fraction, rather than the total N–H content, correlated with tensile strength (r = 0.723) and hardness (r = 0.732). Because all formulations share a 17 wt% hard segment, R = 1.02, a single PPCDL molar mass, and a single heterocyclic modifier loading, the proposed design rules should be regarded as qualitative guidelines whose transferability remains to be validated.
Related
- Functionalization of strong C(sp3)–H bonds in the presence of weak C(sp3)–H bonds enables the block-selective modification of thermoplastic elastomers
- Deformation-Aware Monte Carlo Assessment of a Bi2O3/Thermoplastic Polyurethane Shielding Surrogate Under Tensile Strain and Local Thickness Loss
- Ion Pairing and Electrochemical Behavior of Al(OTf)3 in Propylene Carbonate Bilal Overton
- Study on the coupling reaction of mixed dibasic acid dimethyl esters with propylene carbonate catalyzed by diacidic ionic liquids
- Mechanical performance and eco-efficiency of thermoplastic polyurethane composites reinforced with recycled tire rubber
BibTeX
@article{li2026rigidflexible,
title = {{Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers}},
author = {Bingru Li and Siyu Zhao and Shuanjin Wang and Min Xiao and Zhuofeng Ke and Yuezhong Meng},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18232944},
url = {https://www.mdpi.com/2073-4360/18/23/2944},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers
AU - Bingru Li
AU - Siyu Zhao
AU - Shuanjin Wang
AU - Min Xiao
AU - Zhuofeng Ke
AU - Yuezhong Meng
PY - 2026
DA - 2026/11/24
JO - Polymers
DO - 10.3390/polym18232944
UR - https://www.mdpi.com/2073-4360/18/23/2944
AB - Poly(propylene carbonate) diol (PPCDL) can incorporate CO2 directly into the soft segment of a thermoplastic polyurethane (TPU); however, its rigid and strongly polar carbonate backbone suppresses microphase separation, so lower hardness is usually achieved only at the expense of tensile strength. Herein, this trade-off was addressed by molecular design rather than formulation adjustment within this fixed formulation window. By utilizing a rigid–flexible synergetic strategy, six heterocyclic siloxane modifiers bearing triazole, thiadiazole, or aniline pendants, along with three amino-terminated poly(dimethylsiloxane) (PDMS) controls, were incorporated into PPCDL-based TPUs as chain-extending segments via a torque-rheometer-assisted bulk process at a fixed hard-segment content of 17 wt% and a [NCO]/[OH] ratio of 1.02. Each modifier couples a flexible siloxane spacer with heterocyclic hydrogen-bonding moieties, and the N–H donor and sp2-hybridized nitrogen acceptor counts were explicitly enumerated. The long-chain triazole modifier L2 afforded the most balanced elastomer, with a Shore A hardness of 76, a tensile strength of 5.71 ± 0.44 MPa, and an elongation at break of 892 ± 54%; these values exceeded those of the best PDMS control (4.36 ± 0.33 MPa, 621 ± 0.97%, 80 Shore A) in all evaluated metrics, without any petroleum-based polyol. Gaussian deconvolution of the N–H stretching band showed that the ordered hydrogen-bonded fraction, rather than the total N–H content, correlated with tensile strength (r = 0.723) and hardness (r = 0.732). Because all formulations share a 17 wt% hard segment, R = 1.02, a single PPCDL molar mass, and a single heterocyclic modifier loading, the proposed design rules should be regarded as qualitative guidelines whose transferability remains to be validated.
SN - 2073-4360
ER -