Thickness-dependent crack suppression and wrinkle formation in freestanding BaTiO3 membranes

Abstract

Freestanding ferroelectric oxide membranes offer a promising route toward silicon-integrated low-power electronic and memory devices, but reproducible membrane quality remains challenging, particularly in ultrathin BaTiO3 (BTO), where cracking and wrinkling hinder integration. Here, we show that crack and wrinkle formation in released BaTiO3 membranes can be tuned by jointly controlling oxide thickness and polymer support thickness. Reducing the BaTiO3 thickness from 15 nm to 5 nm suppresses large-area, optically visible cracking across the analysed regions, but promotes dense nanoscale wrinkling, revealing a trade-off between fracture mitigation and morphological instability. In 10 nm BaTiO3 membranes, polymer support thickness further modulates wrinkling, with an intermediate thickness reducing wrinkle density. Piezoresponse force microscopy reveals time-dependent evolution of written contrast after release, indicating that apparent ferroelectric response is influenced by polarization switching, post-release morphology, interfacial contact, charge screening, and strain relaxation. These results establish processing guidelines for integrating freestanding ferroelectrics into future devices.

Versions

Related

  1. Phase-selective growth of water-soluble strontium aluminate via sputtering deposition for freestanding oxide membranes
    Evgenios Stylianidis, Marie Dallocchio, Bernat Mundet +6
    arXivPreprintCC BY-NC-ND 4.0Full textCondensed matterarXiv
  2. Freestanding Antiferromagnetic Oxide Membranes: Synthesis and Characterization of Cr2O3
    Ella Blake, Tiffany C. Wang, Yi Cui +9
    arXivPreprintarXiv licenceFull textCondensed matterarXiv
  3. Non-steady diffusion and adsorption of organic micropollutants in ion-exchange membranes: effect of the membrane thickness
    Malgorzata Roman, Pawel Roman, Rhea Verbeke +9
    iSciencePeer-reviewedCC BY-NC-NDFull text17 citedCondensed matterHAL
  4. Activity-induced emergent flatness, instabilities and pattern formation in fluid membranes
    Debayan Jana, Astik Haldar, Abhik Basu
    arXivPreprintCC BY 4.0Full textStatistical & nonlinear physicsarXiv
  5. Thickness-Dependent Spintronic Terahertz Emission in MBE-Grown PtTe2: From Semiconductor to Type-II Dirac Semimetal
    Rahul Sharma, Sylvain Massabeau, Armando Pezo +13
    Nano LettersPeer-reviewedLicence not statedCondensed matterHAL
BibTeX
@misc{mandal2026thicknessdependent,
  title = {{Thickness-dependent crack suppression and wrinkle formation in freestanding BaTiO3 membranes}},
  author = {Rajesh Mandal and Ajay Kumar and Nini Pryds},
  howpublished = {arXiv},
  year = {2026},
  month = jul,
  doi = {10.48550/arxiv.2607.20054},
  eprint = {2607.20054},
  archivePrefix = {arXiv},
  url = {https://arxiv.org/abs/2607.20054},
  note = {CC BY 4.0},
}
RIS
TY  - UNPB
TI  - Thickness-dependent crack suppression and wrinkle formation in freestanding BaTiO3 membranes
AU  - Rajesh Mandal
AU  - Ajay Kumar
AU  - Nini Pryds
PY  - 2026
DA  - 2026/07/22
PB  - arXiv
DO  - 10.48550/arxiv.2607.20054
UR  - https://arxiv.org/abs/2607.20054
AB  - Freestanding ferroelectric oxide membranes offer a promising route toward silicon-integrated low-power electronic and memory devices, but reproducible membrane quality remains challenging, particularly in ultrathin BaTiO3 (BTO), where cracking and wrinkling hinder integration. Here, we show that crack and wrinkle formation in released BaTiO3 membranes can be tuned by jointly controlling oxide thickness and polymer support thickness. Reducing the BaTiO3 thickness from 15 nm to 5 nm suppresses large-area, optically visible cracking across the analysed regions, but promotes dense nanoscale wrinkling, revealing a trade-off between fracture mitigation and morphological instability. In 10 nm BaTiO3 membranes, polymer support thickness further modulates wrinkling, with an intermediate thickness reducing wrinkle density. Piezoresponse force microscopy reveals time-dependent evolution of written contrast after release, indicating that apparent ferroelectric response is influenced by polarization switching, post-release morphology, interfacial contact, charge screening, and strain relaxation. These results establish processing guidelines for integrating freestanding ferroelectrics into future devices.
ER  -