The Synthesis of Nano-Mg(OH)2 from Lightly Calcined Magnesite Powder via an Ammonia Circulation Route Using Ammonium Bisulfate as a Leaching Agent
- 1Key Laboratory of Chemical Additive Synthesis and Separation, Yingkou Institute of Technology, Yingkou 115014, China
- 2Key Laboratory of Industrial Ecology and Environmental Engineering (Ministry of Education, China), School of Environmental Science and Technology, Dalian University of Technology, Dalian 116024, China
- 3Center for Environmental Technology Research and Experiment, Hebei University of Environmental Engineering, Qinhuangdao 066102, China
Abstract
This study proposes an innovative and environmentally friendly process for synthesizing hexagonal nanosheet-like magnesium hydroxide (Nano-Mg(OH)2) from lightly calcined magnesite powder via ammonium bisulfate leaching–ammonia precipitation combined with ammonia recycling. Under single-factor condition optimization, when the Mg2+ concentration was 0.88 mol/L, the temperature was 50 °C, the time was 1 h, and n(NH3):n(Mg) was 6.03:1, the precipitation rate of Mg(OH)2 reached 88.1%, and the product was confirmed as Mg(OH)2 via XRD and FTIR. In the ammonia recycling experiment (4 g light-burned powder, 50 mL ammonium bisulfate solution), the generated ammonia solution was directly introduced into the previous cycle’s leaching filtrate. The Mg(OH)2 conversion rate reached 74~82.2%. SEM revealed that recycling significantly improved product morphology and dispersibility. The first-cycle product had thicker hexagonal nanosheets (200~500 nm) with uneven agglomerates, while the second-cycle product exhibited thin nanosheets with uniform spherical agglomerates. SEM-EDS mapping showed that Ca, Fe, and Mn fell below detection limits, Al remained extremely low, and Mg content increased with cycle number, with no impurity accumulation in the closed-loop system. This process enables ammonia recycling, reduces reagent consumption and environmental impact, and offers a feasible pathway for the green utilization of lightly calcined magnesite powder and cleaner Nano-Mg(OH)2 production.
Related
- Synthesis of Atomically Precise Pt1Ag34 Bimetallic Nanoclusters and Their Catalytic Performance in the Thermal Decomposition of Ammonium Perchlorate
- Synthesis and crystal structure of tetrakis(ethylammonium) heptaiodide(3−) iodide
- Synthesis of anisotropic silver-coated nanoworms for sensitive SERS detection of crystal violet and ammonium nitrate
- Bisulfate-mediated selective methane oxidation under mild aqueous conditions
- Multiscale insights into the role of hydrated lime content in flash-calcined binders: Linking hydration kinetics, calcium silicate hydrate structure and mechanical performance
BibTeX
@article{duan2026synthesis,
title = {{The Synthesis of Nano-Mg(OH)2 from Lightly Calcined Magnesite Powder via an Ammonia Circulation Route Using Ammonium Bisulfate as a Leaching Agent}},
author = {Xiumei Duan and Chao Wang and Lin Zhang and Yue Zhang and Hai Liang},
journal = {Molecules},
year = {2026},
month = nov,
doi = {10.3390/molecules31224084},
url = {https://www.mdpi.com/1420-3049/31/22/4084},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - The Synthesis of Nano-Mg(OH)2 from Lightly Calcined Magnesite Powder via an Ammonia Circulation Route Using Ammonium Bisulfate as a Leaching Agent
AU - Xiumei Duan
AU - Chao Wang
AU - Lin Zhang
AU - Yue Zhang
AU - Hai Liang
PY - 2026
DA - 2026/11/12
JO - Molecules
DO - 10.3390/molecules31224084
UR - https://www.mdpi.com/1420-3049/31/22/4084
AB - This study proposes an innovative and environmentally friendly process for synthesizing hexagonal nanosheet-like magnesium hydroxide (Nano-Mg(OH)2) from lightly calcined magnesite powder via ammonium bisulfate leaching–ammonia precipitation combined with ammonia recycling. Under single-factor condition optimization, when the Mg2+ concentration was 0.88 mol/L, the temperature was 50 °C, the time was 1 h, and n(NH3):n(Mg) was 6.03:1, the precipitation rate of Mg(OH)2 reached 88.1%, and the product was confirmed as Mg(OH)2 via XRD and FTIR. In the ammonia recycling experiment (4 g light-burned powder, 50 mL ammonium bisulfate solution), the generated ammonia solution was directly introduced into the previous cycle’s leaching filtrate. The Mg(OH)2 conversion rate reached 74~82.2%. SEM revealed that recycling significantly improved product morphology and dispersibility. The first-cycle product had thicker hexagonal nanosheets (200~500 nm) with uneven agglomerates, while the second-cycle product exhibited thin nanosheets with uniform spherical agglomerates. SEM-EDS mapping showed that Ca, Fe, and Mn fell below detection limits, Al remained extremely low, and Mg content increased with cycle number, with no impurity accumulation in the closed-loop system. This process enables ammonia recycling, reduces reagent consumption and environmental impact, and offers a feasible pathway for the green utilization of lightly calcined magnesite powder and cleaner Nano-Mg(OH)2 production.
SN - 1420-3049
ER -