Bismuth-guided cavity confinement breaks the stability–utilization trade-off in zinc powder anodes
- 1Guangxi Key Laboratory of Electrochemical and Magneto-chemical Functional Materials, Guilin University of Technology Guilin 541004 China
- 2Centre for Atomaterials and Nanomanufacturing (CAN), School of Science, RMIT University Melbourne VIC 3000 Australia
Abstract
The practical application of aqueous zinc-ion batteries (AZIBs) is severely hindered by the poor reversibility of the Zn anode, which stems from a self-amplifying cycle involving dendrite growth, interfacial side reactions, and electrically isolated “dead Zn” formation. Here, we report a spray-assembled three-dimensional copper mesh-supported particulate Zn anode, in which Zn particles are encapsulated by an inner bismuth interlayer and an outer carbon confinement shell (3D-C/Bi@Zn-p). Unlike conventional surface stabilization strategies, this surface-engineered architecture enables a unique interface-guided, cavity-confined inward deposition mechanism. During stripping, Zn is selectively extracted from the particle core, leaving behind a robust bismuth–carbon composite shell embedded with isolated internal cavities. In the subsequent plating step, the passivated carbon outer layer effectively suppresses parasitic reactions and prevents Zn nucleation on the external surface, while the inner bismuth layer provides a highly zincophilic interface that kinetically directs Zn2+ to undergo plating exclusively in the cavity interior. Consequently, Zn plating is spatially confined within isolated cavities, effectively suppressing outward dendrite propagation and eliminating the risk of short circuits. Benefiting from this cavity-confined inward deposition behavior, the 3D-C/Bi@Zn-p anode delivers a coulombic efficiency approaching 100% and enables record-high stable cycling for over 10 000 h at 1 mA cm−2 under high zinc utilization of 10.8%. Notably, stable Zn plating/stripping can still be maintained at an ultrahigh Zn utilization of 108%, far beyond the <1% Zn utilization commonly employed in most laboratory-scale studies. Furthermore, when paired with an oxygen-deficient V2O5−x cathode, the full cell delivers 211.6 Wh kg−1 and 81.2% capacity retention after 1000 cycles under lean-anode conditions (N/P = 2.4, ∼30.3% Zn utilization), outperforming most reported AZIBs. This interface-guided cavity-confined inward deposition strategy establishes a new spatial confinement paradigm for reversible metal anodes.
Related
- Turning NOx Pollutants into Green Ammonia Fuel via COF Cavity Confinement
- AI-guided optimization and eco-friendly assessment of in lab stability-indicating HPLC method for empagliflozin and sitagliptin in combined pharmaceutical dosage form
- Evaluation of a bismuth-ellagic acid metal-organic framework for the prophylaxis of inflammatory disorders
- Cyclic ester insertion into a bismuth–amide bond: isolable molecular models for ROP initiation
- A Nano-Bismuth–Silicone Polymer Composite as Shielding for X-Rays in Extreme-Environment Applications: Experimental and Simulation Studies
BibTeX
@article{jiang2026bismuthguided,
title = {{Bismuth-guided cavity confinement breaks the stability–utilization trade-off in zinc powder anodes}},
author = {Yunxuan Jiang and Ziyuan Lan and Can Li and Xiaoning Li and Bo-Tian Liu},
journal = {Chemical Science},
year = {2026},
month = sep,
doi = {10.1039/d6sc05962g},
url = {https://doi.org/10.1039/d6sc05962g},
note = {CC BY-NC 3.0},
}
RIS
TY - JOUR
TI - Bismuth-guided cavity confinement breaks the stability–utilization trade-off in zinc powder anodes
AU - Yunxuan Jiang
AU - Ziyuan Lan
AU - Can Li
AU - Xiaoning Li
AU - Bo-Tian Liu
PY - 2026
DA - 2026/09/04
JO - Chemical Science
DO - 10.1039/d6sc05962g
UR - https://doi.org/10.1039/d6sc05962g
AB - The practical application of aqueous zinc-ion batteries (AZIBs) is severely hindered by the poor reversibility of the Zn anode, which stems from a self-amplifying cycle involving dendrite growth, interfacial side reactions, and electrically isolated “dead Zn” formation. Here, we report a spray-assembled three-dimensional copper mesh-supported particulate Zn anode, in which Zn particles are encapsulated by an inner bismuth interlayer and an outer carbon confinement shell (3D-C/Bi@Zn-p). Unlike conventional surface stabilization strategies, this surface-engineered architecture enables a unique interface-guided, cavity-confined inward deposition mechanism. During stripping, Zn is selectively extracted from the particle core, leaving behind a robust bismuth–carbon composite shell embedded with isolated internal cavities. In the subsequent plating step, the passivated carbon outer layer effectively suppresses parasitic reactions and prevents Zn nucleation on the external surface, while the inner bismuth layer provides a highly zincophilic interface that kinetically directs Zn2+ to undergo plating exclusively in the cavity interior. Consequently, Zn plating is spatially confined within isolated cavities, effectively suppressing outward dendrite propagation and eliminating the risk of short circuits. Benefiting from this cavity-confined inward deposition behavior, the 3D-C/Bi@Zn-p anode delivers a coulombic efficiency approaching 100% and enables record-high stable cycling for over 10 000 h at 1 mA cm−2 under high zinc utilization of 10.8%. Notably, stable Zn plating/stripping can still be maintained at an ultrahigh Zn utilization of 108%, far beyond the <1% Zn utilization commonly employed in most laboratory-scale studies. Furthermore, when paired with an oxygen-deficient V2O5−x cathode, the full cell delivers 211.6 Wh kg−1 and 81.2% capacity retention after 1000 cycles under lean-anode conditions (N/P = 2.4, ∼30.3% Zn utilization), outperforming most reported AZIBs. This interface-guided cavity-confined inward deposition strategy establishes a new spatial confinement paradigm for reversible metal anodes.
SN - 2041-6520
SN - 2041-6539
ER -