Abstract
Corrosion-induced degradation remains a major limitation to the long-term performance of frictional ground-support elements in underground mines, yet the durability of recently developed self-swelling Split-sets remains poorly understood. This study investigates their time-dependent anchorage response under a non-corrosive air control, pure water, pH 3 H₂SO₄ solution, and 6 wt.% Na₂SO₄ solution for up to 90 d using pull-out tests, apparent mass loss measurements, X-ray diffraction analysis and scanning electron microscopy. Under aqueous exposure, a distinct two-stage response was observed: mean peak load increased during the first 14 d and subsequently decreased with prolonged exposure. After 90 d, mean peak load decreased by 24.71%, 30.52%, and 38.59% in pure water, pH 3 H₂SO₄, and 6 wt.% Na₂SO₄, respectively, relative to the 90 d non-corrosive air control. At later exposure durations, aqueous exposure also shifted the governing failure mode from steel-tube rupture to interfacial sliding. Under aqueous exposure, semi-quantitative XRD estimates of relative Ca(OH)₂ content increased during the first 14 d and subsequently decreased, while mean apparent mass loss generally increased. Nevertheless, 90 d mean peak loads remained approximately 3.95–4.87 times those of conventional Split-sets and 1.24–1.48 times those of grouted Split-sets. These results are consistent with a combined influence of early hydration-related strengthening and subsequent exposure-induced degradation; however, the individual contributions of steel corrosion and self-swelling-agent deterioration were not separately quantified. The findings support durability assessment and ground-support selection under the investigated corrosive laboratory conditions.
Related
- Degradation Mechanisms of Concrete in Underground Coal Mine Water Tanks Subjected to Sulphate Attack
- Rock Mass Damage Evolution and Mechanisms of Deformation and Failure in the Intersecting Cavern Complex of a Large Underground Hydropower Powerhouse
- A multivariate approach to estimate the degradation age of plastics in marine environments
- Comparative Study on Photoinhibition Characteristics and Adaptation Mechanisms of New Current-Year Needles of Pinus densiflora var. zhangwuensis and Pinus sylvestris var. mongolica in Sandy Land Environments
- Multi-omics reveals accumulation mechanisms underlying differences in sesquiterpenoid content across different growth environments of Atractylodes macrocephala rhizome
BibTeX
@article{huang2026anchorage,
title = {{Anchorage Degradation and Failure Mechanisms of Self-Swelling Split-Sets Under Corrosive Underground Mine Environments}},
author = {Menglong Huang and Shuai Xu and Fidelis Suorineni and Donghui Li and Zhengming Yang and Qingyu Zhu},
journal = {Applied Sciences},
year = {2026},
month = nov,
doi = {10.3390/app162211291},
url = {https://doi.org/10.3390/app162211291},
note = {CC BY},
}
RIS
TY - JOUR
TI - Anchorage Degradation and Failure Mechanisms of Self-Swelling Split-Sets Under Corrosive Underground Mine Environments
AU - Menglong Huang
AU - Shuai Xu
AU - Fidelis Suorineni
AU - Donghui Li
AU - Zhengming Yang
AU - Qingyu Zhu
PY - 2026
DA - 2026/11/25
JO - Applied Sciences
DO - 10.3390/app162211291
UR - https://doi.org/10.3390/app162211291
AB - Corrosion-induced degradation remains a major limitation to the long-term performance of frictional ground-support elements in underground mines, yet the durability of recently developed self-swelling Split-sets remains poorly understood. This study investigates their time-dependent anchorage response under a non-corrosive air control, pure water, pH 3 H₂SO₄ solution, and 6 wt.% Na₂SO₄ solution for up to 90 d using pull-out tests, apparent mass loss measurements, X-ray diffraction analysis and scanning electron microscopy. Under aqueous exposure, a distinct two-stage response was observed: mean peak load increased during the first 14 d and subsequently decreased with prolonged exposure. After 90 d, mean peak load decreased by 24.71%, 30.52%, and 38.59% in pure water, pH 3 H₂SO₄, and 6 wt.% Na₂SO₄, respectively, relative to the 90 d non-corrosive air control. At later exposure durations, aqueous exposure also shifted the governing failure mode from steel-tube rupture to interfacial sliding. Under aqueous exposure, semi-quantitative XRD estimates of relative Ca(OH)₂ content increased during the first 14 d and subsequently decreased, while mean apparent mass loss generally increased. Nevertheless, 90 d mean peak loads remained approximately 3.95–4.87 times those of conventional Split-sets and 1.24–1.48 times those of grouted Split-sets. These results are consistent with a combined influence of early hydration-related strengthening and subsequent exposure-induced degradation; however, the individual contributions of steel corrosion and self-swelling-agent deterioration were not separately quantified. The findings support durability assessment and ground-support selection under the investigated corrosive laboratory conditions.
SN - 2076-3417
ER -