Skip to content
DraconiticResearch
Search Sources API
276,906 studies31 sourcesUpdated 20 min ago
Peer-reviewedCC BY 4.0Nanomaterials

A Systematic Analysis of the Influence of Structure on Electrochemical Behavior Based on RDE and MEA Data for a Series of Commercial Pt/C Catalysts

4 more authors
4 affiliations
  1. 1Faculty of Chemistry, Southern Federal University, 344090 Rostov-on-Don, Russia
  2. 2Prometheus R&D LLC, 4g/36 Zhmaylova St., 344091 Rostov-on-Don, Russia
  3. 3Federal Research Center the Southern Scientific Center of the Russian Academy of Sciences (SSC RAS), 41 Chekhov Ave., 344006 Rostov-on-Don, Russia
  4. 4Research Institute of Physical Organic Chemistry, Southern Federal University, 194/2 St., 344090 Rostov-on-Don, Russia

Abstract

A systematic evaluation was carried out for the commercial Pt/C electrocatalyst series “PM” (Prometheus R&D LLC) with a platinum mass fraction from 5 to 70 wt.%. Materials with a Pt content of 5–40 wt.% were supported on Vulcan XC-72 carbon, while those with 50–70 wt.% were supported on a highly porous KetjenBlack EC-300J support. The composition, microstructure, electrochemically active surface area (ESA), oxygen reduction reaction (ORR) activity, and stability of the catalysts were studied using X-ray diffraction, TEM/HRTEM, TGA/DSC, cyclic voltammetry, CO-stripping, linear sweep voltammetry with a rotating disk electrode (RDE), and membrane electrode assembly (MEA) testing. It was shown that the average size of Pt nanoparticles (NPs) is 2.1–2.9 nm according to TEM data and 1.6–3.2 nm by XRD; it is controlled predominantly by the wet-synthesis stage rather than by the type of carbon support. With increasing Pt loading, a nonlinear decrease in ESA and mass activity in ORR is observed; the highest mass activity is demonstrated by PM20, while PM30-PM60 catalysts have similar values—328–394 A/g (Pt) and ESA up to 94 m2/g (Pt). The transition to KetjenBlack EC-300J support allows maintaining a uniform distribution of nanoparticles at high loadings and enhances the stability of the materials. The PM series catalysts are characterized by comparable or higher ESA and ORR mass activity than those of HiSPEC4000. In MEA tests, PM30-PM60 catalysts provide a maximum power density of up to 1000 mW/cm2 at a platinum utilization of 0.55–0.72. After durability testing, the loss of maximum power for materials on Vulcan XC-72 is 30–45%, whereas for PM50 and PM60 on KetjenBlack EC-300J it is 9–10%, with a residual power density of more than 2000 W/g(Pt) and more than 900 mW/cm2. It was established that the type of carbon support largely determines the stability of the catalysts, owing to differences in the degradation of both catalyst activity and the transport properties of the catalyst layers, as assessed by EIS. The obtained data can serve as reference data when comparing commercial and laboratory Pt/C catalysts for proton exchange membrane fuel cells (PEMFCs).

Related

  1. From hard carbon to activated carbon: influence of surface area and pore structure on the electrochemical performance of coconut rachis-derived supercapacitor electrodes
    Devu Bindhu, M. S. Gayathri, Anju Ramachandran +3
    Scientific ReportsPeer-reviewedCC BY-NC-ND 4.0Full textMaterials & polymersCrossref
  2. Acid Sites, Pore Architecture and Catalytic Function in Commercial Clay Catalysts
    Ouahiba Madjeda Mecelti, Maryann Uzochukwu, Tomo Suzuki-Muresan +2
    Applied Catalysis A: GeneralPreprintLicence not statedFull textCatalysisEnvironmental science & pollutionHAL
  3. Examining Copper Lead Surface Alloys as Potential Catalysts for the Electrochemical Carbon Dioxide Reduction
    Oliver Kratz, Axel Groß
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  4. Probing electrochemical phenomena in commercial pouch cells using a multimodal magnetic resonance approach
    Konstantin Romanenko, Nikolai Avdievich
    Journal of Materials Chemistry APeer-reviewedCC BY-NC2 citedPhysical chemistryHAL
  5. Heterogeneous Catalysts as Electrochemical Cells: Completing the Circuit using Proton Buffers in Nonaqueous Media
    Patrick Q. Kelly, Woonjin Jang, Ian J. Garvey +2
    ChemRxivPreprintCC BYFull textElectrochemistry & energyChemRxiv
BibTeX
@article{moguchikh2026systematic,
  title = {{A Systematic Analysis of the Influence of Structure on Electrochemical Behavior Based on RDE and MEA Data for a Series of Commercial Pt/C Catalysts}},
  author = {Elizaveta Moguchikh and Angelina Pavlets and Kirill Paperzh and Alina Nevelskaya and Yegor Beskopylny and Dmitry Mauer and Ilya Kantsypa and Yana Astravukh and Alina Khudoley and Anna Gavrilova and Ilya Pankov and Mikhail Tolstunov and Danil Alekseenko and Anastasia Alekseenko and Vladimir Guterman and Sergey Belenov},
  journal = {Nanomaterials},
  year = {2026},
  month = nov,
  doi = {10.3390/nano16231544},
  url = {https://www.mdpi.com/2079-4991/16/23/1544},
  note = {CC BY 4.0},
}
RIS
TY  - JOUR
TI  - A Systematic Analysis of the Influence of Structure on Electrochemical Behavior Based on RDE and MEA Data for a Series of Commercial Pt/C Catalysts
AU  - Elizaveta Moguchikh
AU  - Angelina Pavlets
AU  - Kirill Paperzh
AU  - Alina Nevelskaya
AU  - Yegor Beskopylny
AU  - Dmitry Mauer
AU  - Ilya Kantsypa
AU  - Yana Astravukh
AU  - Alina Khudoley
AU  - Anna Gavrilova
AU  - Ilya Pankov
AU  - Mikhail Tolstunov
AU  - Danil Alekseenko
AU  - Anastasia Alekseenko
AU  - Vladimir Guterman
AU  - Sergey Belenov
PY  - 2026
DA  - 2026/11/26
JO  - Nanomaterials
DO  - 10.3390/nano16231544
UR  - https://www.mdpi.com/2079-4991/16/23/1544
AB  - A systematic evaluation was carried out for the commercial Pt/C electrocatalyst series “PM” (Prometheus R&D LLC) with a platinum mass fraction from 5 to 70 wt.%. Materials with a Pt content of 5–40 wt.% were supported on Vulcan XC-72 carbon, while those with 50–70 wt.% were supported on a highly porous KetjenBlack EC-300J support. The composition, microstructure, electrochemically active surface area (ESA), oxygen reduction reaction (ORR) activity, and stability of the catalysts were studied using X-ray diffraction, TEM/HRTEM, TGA/DSC, cyclic voltammetry, CO-stripping, linear sweep voltammetry with a rotating disk electrode (RDE), and membrane electrode assembly (MEA) testing. It was shown that the average size of Pt nanoparticles (NPs) is 2.1–2.9 nm according to TEM data and 1.6–3.2 nm by XRD; it is controlled predominantly by the wet-synthesis stage rather than by the type of carbon support. With increasing Pt loading, a nonlinear decrease in ESA and mass activity in ORR is observed; the highest mass activity is demonstrated by PM20, while PM30-PM60 catalysts have similar values—328–394 A/g (Pt) and ESA up to 94 m2/g (Pt). The transition to KetjenBlack EC-300J support allows maintaining a uniform distribution of nanoparticles at high loadings and enhances the stability of the materials. The PM series catalysts are characterized by comparable or higher ESA and ORR mass activity than those of HiSPEC4000. In MEA tests, PM30-PM60 catalysts provide a maximum power density of up to 1000 mW/cm2 at a platinum utilization of 0.55–0.72. After durability testing, the loss of maximum power for materials on Vulcan XC-72 is 30–45%, whereas for PM50 and PM60 on KetjenBlack EC-300J it is 9–10%, with a residual power density of more than 2000 W/g(Pt) and more than 900 mW/cm2. It was established that the type of carbon support largely determines the stability of the catalysts, owing to differences in the degradation of both catalyst activity and the transport properties of the catalyst layers, as assessed by EIS. The obtained data can serve as reference data when comparing commercial and laboratory Pt/C catalysts for proton exchange membrane fuel cells (PEMFCs).
SN  - 2079-4991
ER  -