Temperature Flips the Sign of the Hydrogen Response in Nanogranular Palladium Networks

Abstract

In nanogranular palladium networks, hydrogen uptake has two opposing effects on electrical resistance. Absorbed hydrogen scatters electrons within the particles, raising their resistance, while particle expansion narrows the gaps between them and lowers the junction resistance. Such networks are widely studied as resistive hydrogen sensors, and the sign of their net response is usually treated as a fixed property of the architecture. In networks grown by atomic layer deposition on macroporous silicon, we show that changing the operating temperature can reverse this sign at a fixed hydrogen concentration. A thermodynamic model indicates that scattering contributes less as temperature rises, allowing sub-angstroem changes in gap width to dominate. Where the two effects cancel, the network absorbs hydrogen yet gives the same reading as in hydrogen-free gas, so a leak could escape detection. Between 25 and 40 degrees Celsius, this cancellation point is predicted to rise over tenfold, crossing reported leak-alarm setpoints. At 55 degrees Celsius, the measured response stays negative but passes through a minimum, so a concentration above a setpoint can mimic one below it. Annealing at 200 degrees Celsius alters the calibration and turns the room-temperature response negative at the lowest concentration tested. Quantitative sensing therefore requires a defined thermal pretreatment and an operating temperature giving distinct signals across the intended concentration range. Response polarity becomes an operating parameter rather than a fixed property. More broadly, any nanoparticle network whose particles deform on sorption may show the same temperature-dependent competition between transport within and between particles, with implications for sensors and switches beyond palladium-hydrogen.

Related

  1. Assessment of machine-learned vs. classical/quantum atomistic simulations for predicting palladium-hydrogen materials
    Yifan Yao, Qiang Xu, James D. Symons Galassi +1
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  2. Grain Boundary and Stress Evolution during Thin Film Growth: Key Factors Governing the Resistive Hydrogen-Sensing Characteristics of Palladium Thin Films
    Yizhou Jiao, Weijiang Chen, Zheng Tang +5
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  3. Room temperature Suzuki coupling of aryl iodides, bromides, and chlorides using a heterogeneous carbon nanotube-palladium nanohybrid catalyst
    Dhanaji Jawale, Edmond Gravel, Caroline Boudet +5
    Catalysis Science & TechnologyPeer-reviewedCC BYFull text65 citedOrganic chemistryHAL
  4. Nanoporous palladium as a sustainable and temperature-adaptive nanozyme with oxidase-like activity for the detection of antioxidants
    Chuting Zhang, Xue Liu, Yating Fan +3
    RSC AdvancesPeer-reviewedCC BY 3.0Full textMaterials & polymersPMC
  5. Deciphering Electrochemical Generation, Transport, and Reactivity of Hydrogen Species in the Electrochemical Palladium Membrane Reactor.
    Samuel J Shin, Su Bin Roh, Hyun-Tak Kim +4
    Advanced science (Weinheim, Baden-Wurttemberg, Germany)Peer-reviewedCC BYFull textOrganic chemistryEurope PMC
BibTeX
@misc{alkazaz2026temperature,
  title = {{Temperature Flips the Sign of the Hydrogen Response in Nanogranular Palladium Networks}},
  author = {Niclas Alkazaz and Robert Zierold and Patrick Huber},
  howpublished = {arXiv},
  year = {2026},
  month = nov,
  doi = {10.48550/arxiv.2611.22877},
  eprint = {2611.22877},
  archivePrefix = {arXiv},
  url = {https://arxiv.org/abs/2611.22877},
  note = {CC BY 4.0},
}
RIS
TY  - UNPB
TI  - Temperature Flips the Sign of the Hydrogen Response in Nanogranular Palladium Networks
AU  - Niclas Alkazaz
AU  - Robert Zierold
AU  - Patrick Huber
PY  - 2026
DA  - 2026/11/17
PB  - arXiv
DO  - 10.48550/arxiv.2611.22877
UR  - https://arxiv.org/abs/2611.22877
AB  - In nanogranular palladium networks, hydrogen uptake has two opposing effects on electrical resistance. Absorbed hydrogen scatters electrons within the particles, raising their resistance, while particle expansion narrows the gaps between them and lowers the junction resistance. Such networks are widely studied as resistive hydrogen sensors, and the sign of their net response is usually treated as a fixed property of the architecture. In networks grown by atomic layer deposition on macroporous silicon, we show that changing the operating temperature can reverse this sign at a fixed hydrogen concentration. A thermodynamic model indicates that scattering contributes less as temperature rises, allowing sub-angstroem changes in gap width to dominate. Where the two effects cancel, the network absorbs hydrogen yet gives the same reading as in hydrogen-free gas, so a leak could escape detection. Between 25 and 40 degrees Celsius, this cancellation point is predicted to rise over tenfold, crossing reported leak-alarm setpoints. At 55 degrees Celsius, the measured response stays negative but passes through a minimum, so a concentration above a setpoint can mimic one below it. Annealing at 200 degrees Celsius alters the calibration and turns the room-temperature response negative at the lowest concentration tested. Quantitative sensing therefore requires a defined thermal pretreatment and an operating temperature giving distinct signals across the intended concentration range. Response polarity becomes an operating parameter rather than a fixed property. More broadly, any nanoparticle network whose particles deform on sorption may show the same temperature-dependent competition between transport within and between particles, with implications for sensors and switches beyond palladium-hydrogen.