Transition-metal-loaded TiO2 catalysts for CO oxidation: metal-dependent activity and surface redox properties
- 1School of Materials Science and Engineering, Northeastern University Shenyang Liaoning 110004 China.
- 2Research Institute of Urbanization and Urban Safety, School of Future Cities, University of Science and Technology Beijing Beijing 100083 China [email protected].
- 3School of Chemical Engineering and Technology, Xi'an Jiaotong University Xi'an Shaanxi 710049 China [email protected].
Abstract
In this work, a series of M/TiO₂ catalysts (M = Fe, Co, Ni, Cu and Zn) were prepared on the same TiO₂ support under consistent impregnation, evaporation and calcination conditions to systematically compare the effects of metal identity on low-temperature CO oxidation. The thermal catalytic activity among the M/TiO₂ catalysts followed the order Cu/TiO₂ > Fe/TiO₂ > Co/TiO₂ > Ni/TiO₂ > Zn/TiO₂. Cu/TiO₂ exhibited the highest activity, which was associated with its favorable low-temperature reducibility, mixed Cu oxidation states, and relatively high proportion of surface adsorbed or defect-related oxygen species. Light-assisted tests showed enhanced CO oxidation over Cu/TiO₂, with the T ₁₀, T ₅₀ and T ₉₀ decreasing from 117, 158 and 180 °C under thermal conditions to 70, 77 and 100 °C under photothermal conditions, respectively. Meanwhile, the apparent activation energy decreased from 41.7 to 30.3 kJ mol⁻¹. In situ DRIFTS under thermal conditions revealed that formate, carboxylate and carbonate species were important surface intermediates in the CO oxidation process over Cu/TiO₂. After gaseous O₂ was removed, these surface species continued to evolve, indicating that oxygen species retained on the catalyst surface could still participate in CO conversion. After O₂ was reintroduced, the accumulated surface intermediates were further oxidized and the reaction gradually returned to equilibrium. These results indicated that surface oxygen species participated in the conversion of adsorbed CO, while gaseous O₂ continuously replenished reactive oxygen species on the catalyst surface.
Related
- Controlling Interfacial and Bulk Charge Transport in Exsolution Catalysts for High-Activity Water Oxidation
- Roles of Ru Loading in Modulating Soot Oxidation Activity and Sulfur Resistance of Ru/Al2O3 Catalysts
- Hybrid Pt/CeO2/TiO2 Catalysts for Low-Temperature Iron(II) Ion Oxidation with Oxygen in Acidic Media
- Selective oxidation of ethanol towards a highly valuable product over industrial and model catalysts
- General Preparation of Nickel-Based Compound/Carbon Nanotube Catalysts for the Urea Oxidation Reaction
BibTeX
@article{chen2026transitionmetalloaded,
title = {{Transition-metal-loaded TiO2 catalysts for CO oxidation: metal-dependent activity and surface redox properties}},
author = {Shanshan Chen and Weimin Huang and Ke-Xin Li and Jiazhuo Chen and Yuanhao Wang and Zhun Hu},
journal = {RSC advances},
year = {2026},
month = nov,
doi = {10.1039/d6ra09728f},
url = {https://europepmc.org/article/PMC/PMC13795230},
note = {CC BY-NC},
}
RIS
TY - JOUR
TI - Transition-metal-loaded TiO2 catalysts for CO oxidation: metal-dependent activity and surface redox properties
AU - Shanshan Chen
AU - Weimin Huang
AU - Ke-Xin Li
AU - Jiazhuo Chen
AU - Yuanhao Wang
AU - Zhun Hu
PY - 2026
DA - 2026/11/24
JO - RSC advances
DO - 10.1039/d6ra09728f
UR - https://europepmc.org/article/PMC/PMC13795230
AB - In this work, a series of M/TiO₂ catalysts (M = Fe, Co, Ni, Cu and Zn) were prepared on the same TiO₂ support under consistent impregnation, evaporation and calcination conditions to systematically compare the effects of metal identity on low-temperature CO oxidation. The thermal catalytic activity among the M/TiO₂ catalysts followed the order Cu/TiO₂ > Fe/TiO₂ > Co/TiO₂ > Ni/TiO₂ > Zn/TiO₂. Cu/TiO₂ exhibited the highest activity, which was associated with its favorable low-temperature reducibility, mixed Cu oxidation states, and relatively high proportion of surface adsorbed or defect-related oxygen species. Light-assisted tests showed enhanced CO oxidation over Cu/TiO₂, with the T ₁₀, T ₅₀ and T ₉₀ decreasing from 117, 158 and 180 °C under thermal conditions to 70, 77 and 100 °C under photothermal conditions, respectively. Meanwhile, the apparent activation energy decreased from 41.7 to 30.3 kJ mol⁻¹. In situ DRIFTS under thermal conditions revealed that formate, carboxylate and carbonate species were important surface intermediates in the CO oxidation process over Cu/TiO₂. After gaseous O₂ was removed, these surface species continued to evolve, indicating that oxygen species retained on the catalyst surface could still participate in CO conversion. After O₂ was reintroduced, the accumulated surface intermediates were further oxidized and the reaction gradually returned to equilibrium. These results indicated that surface oxygen species participated in the conversion of adsorbed CO, while gaseous O₂ continuously replenished reactive oxygen species on the catalyst surface.
SN - 2046-2069
ER -