Skip to content
DraconiticResearch
Search Sources API
182,460 studies31 sourcesUpdated 56 min ago
Peer-reviewedCC BYEnvironmental science & technology

Aerosol-Assisted Metal Poisoning of Cu/SSZ-13 during NH3-SCR Operation.

6 affiliations
  1. 1School of Chemistry and Life Resources, Renmin University of China, Beijing100872, P. R. China.
  2. 2Department of Advanced Methods for Applied Catalysis, Leibniz-Institut für Katalyse e.V. (LIKAT), Rostock18059, Germany.
  3. 3College of Science, China University of Petroleum, Beijing102249, P. R. China.
  4. 4College of Chemistry and Chemical Engineering, Taiyuan University of Technology, Taiyuan030024, P. R. China.
  5. 5School of Petrochemical Engineering, Liaoning Petrochemical University, Fushun113001, P. R. China.
  6. 6State Key Joint Laboratory of Environment Simulation and Pollution Control, School of Environment, Tsinghua University, Beijing100084, P. R. China.

Abstract

Cu/SSZ-13 is a benchmark catalyst for the selective catalytic reduction (SCR) of NOx with NH3 in diesel exhaust aftertreatment, but its activity can be severely impaired by alkali and alkaline-earth metal poisoning. Conventional impregnation of catalysts with such poisons involves introducing metal species prior to catalytic testing. This means that any poisoning that develops concurrently with catalyst operation is not captured. Here, we develop an aerosol-assisted, reaction-coupled poisoning platform that continuously delivers metal-containing aqueous aerosols to SCR catalysts under hydrated NH3-SCR conditions. At nearly identical K loadings, aerosol-assisted poisoning caused substantially greater deactivation of Cu/SSZ-13 than conventional impregnation of the catalyst, with a more pronounced activity loss after poisoning at 400 °C than at 200 °C. The enhanced deactivation was accompanied by a more spatially extensive K distribution, stronger perturbations of the zeolite framework, preferential alteration of 8-membered-ring-associated [Cu(OH)]+-Z species, spectroscopic signatures consistent with CuOx aggregation, and partial neutralization of Brønsted acid sites. Similar pathway- and temperature-dependent deactivation trends were observed for Na-, Mg-, and Ca-poisoned Cu/SSZ-13 and for K-poisoned V2O5-WO3/TiO2. These results establish aerosol-assisted poisoning as a controlled, accelerated approach for evaluating metal-induced deactivation of SCR catalysts under hydrated reaction conditions.

Related

  1. Aerosol-assisted chemical vapour deposition of Zn3P2 films for sodium-ion battery anodes
    Kaiqing Fan, Xueqing Li, Xiang Lian +2
    Dalton transactions (Cambridge, England : 2003)Peer-reviewedCC BYFull textGeneral chemistryEurope PMC
  2. Metal‐Support Interaction Triggered Electronic Reconstruction in Pd/CoN‐Co 4 N Catalysts for Optimizing MEK Oxidation and Poisoning Resistance
    Yadi Wang, Chaoqian Ai, Cai Wang +5
    Advanced SciencePeer-reviewedCC BY12 citedMaterials & polymersOpenAlex
  3. Investigation of Secondary Phase Evolution in LSCF Electrodes during Long-Term SOEC Operation by X‑ray Diffraction and Electron Microscopy Characterizations
    ACS omegaPeer-reviewedCC BY-NC-NDFull textGeneral chemistryEurope PMC
  4. Single-Particle Insight into the Compression of Electrocatalytic Activity Distributions during Catalyst Poisoning.
    Ishaan Shah, Miguel Orozco, Lior Sepunaru
    ACS measurement science auPeer-reviewedCC BY-NC-NDFull textElectrochemistry & energyEurope PMC
  5. Iridium Oxidation-State Dynamics during Transient Operation under PEM Water Electrolysis Single-Cell Conditions Revealed by Time-Resolved Operando XAS
    Kenta Hayashi, Shuji Takahashi, Masanori Inaba +3
    ChemRxivPreprintCC BYElectrochemistry & energyChemRxiv
BibTeX
@article{zhang2026aerosolassisted,
  title = {{Aerosol-Assisted Metal Poisoning of Cu/SSZ-13 during NH3-SCR Operation.}},
  author = {Tao Zhang and Jianning Zhang and Feng Yu and Qi Dong and Jian Liu and Junhua Li and Evgenii V Kondratenko},
  journal = {Environmental science \& technology},
  year = {2026},
  month = oct,
  doi = {10.1021/acs.est.6c07432},
  url = {https://europepmc.org/article/MED/42915947},
  note = {CC BY},
}
RIS
TY  - JOUR
TI  - Aerosol-Assisted Metal Poisoning of Cu/SSZ-13 during NH3-SCR Operation.
AU  - Tao Zhang
AU  - Jianning Zhang
AU  - Feng Yu
AU  - Qi Dong
AU  - Jian Liu
AU  - Junhua Li
AU  - Evgenii V Kondratenko
PY  - 2026
DA  - 2026/10/01
JO  - Environmental science & technology
DO  - 10.1021/acs.est.6c07432
UR  - https://europepmc.org/article/MED/42915947
AB  - Cu/SSZ-13 is a benchmark catalyst for the selective catalytic reduction (SCR) of NOx with NH3 in diesel exhaust aftertreatment, but its activity can be severely impaired by alkali and alkaline-earth metal poisoning. Conventional impregnation of catalysts with such poisons involves introducing metal species prior to catalytic testing. This means that any poisoning that develops concurrently with catalyst operation is not captured. Here, we develop an aerosol-assisted, reaction-coupled poisoning platform that continuously delivers metal-containing aqueous aerosols to SCR catalysts under hydrated NH3-SCR conditions. At nearly identical K loadings, aerosol-assisted poisoning caused substantially greater deactivation of Cu/SSZ-13 than conventional impregnation of the catalyst, with a more pronounced activity loss after poisoning at 400 °C than at 200 °C. The enhanced deactivation was accompanied by a more spatially extensive K distribution, stronger perturbations of the zeolite framework, preferential alteration of 8-membered-ring-associated [Cu(OH)]+-Z species, spectroscopic signatures consistent with CuOx aggregation, and partial neutralization of Brønsted acid sites. Similar pathway- and temperature-dependent deactivation trends were observed for Na-, Mg-, and Ca-poisoned Cu/SSZ-13 and for K-poisoned V2O5-WO3/TiO2. These results establish aerosol-assisted poisoning as a controlled, accelerated approach for evaluating metal-induced deactivation of SCR catalysts under hydrated reaction conditions.
SN  - 0013-936X
SN  - 1520-5851
ER  -