Experimental and Inverse Analysis of Natural Cork Material with Anisotropic Nonlinear Viscoelastic Behavior
- 1Laboratoire Mécatronique (LMT), Faculty of Sciences and Technology, University of Jijel, Jijel 18000, Algeria
- 2Laboratoire de Génie Mécanique-Jijel, University of Jijel, Jijel 18000, Algeria
- 3Department of Materials Science and Engineering, Division of Applied Mechanics, Uppsala University, Box 524, 751 20 Uppsala, Sweden
Abstract
Due to its cellular structure, cork from Quercus suber has significant deformability, showing magnificent recovery after being compressed by 50%. Its mechanical characteristics show dependency on the direction of the external load (anisotropy), making it difficult to estimate recoverable large displacements. Here, the mechanical behavior of cork is investigated under loading–unloading cycles (1–15 MPa) in the radial and non-radial directions. Cork demonstrates higher stiffness and higher residual strain in the radial direction, compared to the softer, buckling-dominated behavior in the non-radial direction. Both directions feature significant cycle-by-cycle softening, suggesting a Mullins-type (recoverable) damage mechanism, with residual strain increasing in both directions. According to the data obtained six months after testing, dimensional recovery demonstrates ongoing recovery with varying percentages depending on the direction (92% against 88% of the original height after six months). It supports the theory of softening from cycle to cycle because the damage is primarily pseudo-elastic and therefore recoverable rather than irreversible. A transversely isotropic hyperelastic constitutive model is enriched with Mullins-type (pseudo-elastic) damage and viscoelasticity. The three-dimensional model is based on engineering applications; all parameters are obtained through inverse analysis of loading–unloading tests. Consequently, this model accounts for the anisotropic behavior and increasing recoverable damage of cork, allowing better prediction of its mechanical performance.
Related
- Anisotropic electron gas in a hyperbolic van der Waals material
- Thermal Aging Behavior of PFA-Insulated Cables for Future Electrified Aircraft: From Material Evolution to Cable-Level Mechanical Response
- Experimental and Numerical Investigation of the Interfacial Bonding in Multi-Material Fused-Filament Fabrication Using Mode-I Fracture Toughness
- Experimental and computational analysis of the nonlinear optical responses of styrylquinoline-functionalized polymers for optoelectronic applications
- Deciphering pH Behavior in Deep Eutectic Solvents: Synergizing Experimental Data and Computational Modeling
BibTeX
@article{yahiaoui2026experimental,
title = {{Experimental and Inverse Analysis of Natural Cork Material with Anisotropic Nonlinear Viscoelastic Behavior}},
author = {Cylia Yahiaoui and Younès Saadallah and Reza Afshar and Kristofer Gamstedt and B. Emek Abali},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18212722},
url = {https://www.mdpi.com/2073-4360/18/21/2722},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - Experimental and Inverse Analysis of Natural Cork Material with Anisotropic Nonlinear Viscoelastic Behavior
AU - Cylia Yahiaoui
AU - Younès Saadallah
AU - Reza Afshar
AU - Kristofer Gamstedt
AU - B. Emek Abali
PY - 2026
DA - 2026/11/02
JO - Polymers
DO - 10.3390/polym18212722
UR - https://www.mdpi.com/2073-4360/18/21/2722
AB - Due to its cellular structure, cork from Quercus suber has significant deformability, showing magnificent recovery after being compressed by 50%. Its mechanical characteristics show dependency on the direction of the external load (anisotropy), making it difficult to estimate recoverable large displacements. Here, the mechanical behavior of cork is investigated under loading–unloading cycles (1–15 MPa) in the radial and non-radial directions. Cork demonstrates higher stiffness and higher residual strain in the radial direction, compared to the softer, buckling-dominated behavior in the non-radial direction. Both directions feature significant cycle-by-cycle softening, suggesting a Mullins-type (recoverable) damage mechanism, with residual strain increasing in both directions. According to the data obtained six months after testing, dimensional recovery demonstrates ongoing recovery with varying percentages depending on the direction (92% against 88% of the original height after six months). It supports the theory of softening from cycle to cycle because the damage is primarily pseudo-elastic and therefore recoverable rather than irreversible. A transversely isotropic hyperelastic constitutive model is enriched with Mullins-type (pseudo-elastic) damage and viscoelasticity. The three-dimensional model is based on engineering applications; all parameters are obtained through inverse analysis of loading–unloading tests. Consequently, this model accounts for the anisotropic behavior and increasing recoverable damage of cork, allowing better prediction of its mechanical performance.
SN - 2073-4360
ER -