Preclinical Assessment of Early Interaction Between Absorbable Poly-4-Hydroxybutyrate Scaffolds and Silicone Breast Implants.
Abstract
Absorbable scaffolds, such as poly-4-hydroxybutyrate (P4HB), are increasingly used in aesthetic breast surgery to support implants. However, the nature and timing of scaffold-implant interactions during early healing remain uncharacterized. The aim of this report was to evaluate whether contact between P4HB scaffolds and silicone implants can cause mechanical weakening of either device or wear-related particulate generation. Two independent studies were performed. An animal study assessed early P4HB scaffold-tissue integration. Characteristics and histology of scaffold explants were compared with native capsules after 4 weeks in a porcine silicone implant model. A separate benchtop study evaluated scaffold and implant mechanical integrity and particulate generation after interactive cyclic loading for 12 weeks, exceeding the in vivo integration period, to conservatively evaluate interaction. Mechanical testing was performed on implants and scaffolds after interaction and compared with nontested devices. Particulate analysis was performed on fluid collected from the bench apparatus. Scaffold-tissue capsules show surface characteristics similar to native tissue capsules, indicating complete integration at 4 weeks. After 12-week benchtop loading, mechanical properties of scaffolds and implants were comparable to controls and met standard specifications for new devices. Particulates were below detection limits. This preclinical study evaluated early scaffold-implant interaction during the period of maximal direct polymer contact and assessed mechanical interactions under worst-case simulated conditions. By 4 weeks in animals, tissue integration limits direct polymer-implant contact. After 12 weeks on the bench, no compromise of implant or scaffold mechanical integrity or detectable particulates was observed under the tested conditions. These findings provide preliminary data and do not address long-term effects. Level of Evidence: 5 (Therapeutic) For image description, please refer to the figure legend and surrounding text.
Related
- Animal Models for Preclinical Evaluation of Bioresorbable Scaffolds and Tissue-Engineered Constructs in Breast Reconstruction.
- Association of Structured Preclinical Phantom Training and OSCE/OSPE-Based Assessment with Endodontic Procedural Complications Among Dental Students: A Retrospective Cohort Study
- 401 genO-hCCR8/hCCL1/hFcγR preclinical mouse model for efficacy assessment of CCR8-targeting agents
- EP18.17 Preclinical assessment of a pH-responsive nanocomposite using a refined orthotopic murine model of glioblastoma resection
- EP09.16 Preclinical Assessment of treatment scheduling for Tumor Treating Fields (TTFields) Applied Concurrently with Radiation Therapy in Glioblastoma
BibTeX
@article{vanhamme2026preclinical,
title = {{Preclinical Assessment of Early Interaction Between Absorbable Poly-4-Hydroxybutyrate Scaffolds and Silicone Breast Implants.}},
author = {Cassandra Vanhamme and Darcy H Gagne and Cameron Bloomquist and Ashley McLaughlin and Diana Catalina Ardila and Tyler Stahl and Catherine C Steele and Amit Badhwar and Sakib F Elahi},
journal = {Aesthetic surgery journal. Open forum},
year = {2026},
month = oct,
doi = {10.1093/asjof/ojag205},
url = {https://europepmc.org/article/MED/43055025},
note = {CC BY},
}
RIS
TY - JOUR
TI - Preclinical Assessment of Early Interaction Between Absorbable Poly-4-Hydroxybutyrate Scaffolds and Silicone Breast Implants.
AU - Cassandra Vanhamme
AU - Darcy H Gagne
AU - Cameron Bloomquist
AU - Ashley McLaughlin
AU - Diana Catalina Ardila
AU - Tyler Stahl
AU - Catherine C Steele
AU - Amit Badhwar
AU - Sakib F Elahi
PY - 2026
DA - 2026/10/21
JO - Aesthetic surgery journal. Open forum
DO - 10.1093/asjof/ojag205
UR - https://europepmc.org/article/MED/43055025
AB - Absorbable scaffolds, such as poly-4-hydroxybutyrate (P4HB), are increasingly used in aesthetic breast surgery to support implants. However, the nature and timing of scaffold-implant interactions during early healing remain uncharacterized. The aim of this report was to evaluate whether contact between P4HB scaffolds and silicone implants can cause mechanical weakening of either device or wear-related particulate generation. Two independent studies were performed. An animal study assessed early P4HB scaffold-tissue integration. Characteristics and histology of scaffold explants were compared with native capsules after 4 weeks in a porcine silicone implant model. A separate benchtop study evaluated scaffold and implant mechanical integrity and particulate generation after interactive cyclic loading for 12 weeks, exceeding the in vivo integration period, to conservatively evaluate interaction. Mechanical testing was performed on implants and scaffolds after interaction and compared with nontested devices. Particulate analysis was performed on fluid collected from the bench apparatus. Scaffold-tissue capsules show surface characteristics similar to native tissue capsules, indicating complete integration at 4 weeks. After 12-week benchtop loading, mechanical properties of scaffolds and implants were comparable to controls and met standard specifications for new devices. Particulates were below detection limits. This preclinical study evaluated early scaffold-implant interaction during the period of maximal direct polymer contact and assessed mechanical interactions under worst-case simulated conditions. By 4 weeks in animals, tissue integration limits direct polymer-implant contact. After 12 weeks on the bench, no compromise of implant or scaffold mechanical integrity or detectable particulates was observed under the tested conditions. These findings provide preliminary data and do not address long-term effects. Level of Evidence: 5 (Therapeutic) For image description, please refer to the figure legend and surrounding text.
SN - 2631-4797
ER -