Rehabilitation of Concrete Pipelines with Invert Voids by Non-Water-Reactive Polymer Grouting: The Interface Expansion Pressure Evolution and Lifting Response
4 affiliations
- 1School of Water Conservancy and Transportation, Zhengzhou University, Zhengzhou 450001, China
- 2School of Mechanics and Civil Engineering, China University of Mining and Technology, Xuzhou 221116, China
- 3State Key Laboratory for Fine Exploration and Intelligent Development of Coal Resources, China University of Mining and Technology, Xuzhou 221116, China
- 4School of Civil Engineering and Transportation, North China University of Water Resources and Electric Power, Zhengzhou 450016, China
Abstract
Invert voids beneath underground concrete pipelines can cause support loss and settlement, while the spatial evolution of interfacial forces generated by confined polymer foaming remains poorly understood. Small-scale curved-interface grouting tests were conducted to investigate the effects of grout density, interface arch height, and circumferential position on local expansion forces, and a quadratic response surface model was developed for force prediction. Full-scale pipeline lifting tests were subsequently performed to investigate the relationship between interfacial expansion and structural displacement. The expansion response exhibited three stages—filling, rapid foaming, and stabilization—with pronounced spatial nonuniformity. Increasing grout density from 0.26 to 0.36 g/cm3 increased the peak expansion force by 58.9–69.7%, whereas increasing arch height from 8.14 to 14.60 mm resulted in an increase of only 5.3–9.2%. The response surface model showed good agreement with the experimental data used for model development (R2 = 0.9896). The full-scale test achieved a pipeline uplift of 50 mm, with the bell section lifting approximately 2.1 times faster than the spigot section during rapid uplift. A simplified equilibrium analysis yielded a theoretical critical grout density of 0.29 g/cm3 for initiating pipe uplift providing a preliminary reference for grouting parameter design and pipeline rehabilitation.
Related
- Nanomaterial-Enabled Flexible Wearable Sensors for Sports Monitoring and Rehabilitation: Material Architectures, Interface Design, and Signal Reliability
- Spontaneous gas film expansion at an oil–water interface
- Experimental Study on the Shear Transfer Resistance of Uncracked Concrete Interfaces Reinforced with GFRP
- Experimental Study on Methane Explosion Suppression in Pipelines by Mixed Systems of Inert Gases (CO2/N2) and HFC-227ea
- Comparison of One-Dimensional and Quasi-Two-Dimensional Friction Models for Hydraulic Transient Response and Energy Dissipation in Viscoelastic Pipelines at Different Water Temperatures
BibTeX
@article{li2026rehabilitation,
title = {{Rehabilitation of Concrete Pipelines with Invert Voids by Non-Water-Reactive Polymer Grouting: The Interface Expansion Pressure Evolution and Lifting Response}},
author = {Chenguang Li and Zhanyang Lin and Mingrui Du and Xupei Yao and Shiming Liu and Shiao Chen and Haijian Su and Liang Chen and Yanke Shi},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18222828},
url = {https://www.mdpi.com/2073-4360/18/22/2828},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - Rehabilitation of Concrete Pipelines with Invert Voids by Non-Water-Reactive Polymer Grouting: The Interface Expansion Pressure Evolution and Lifting Response
AU - Chenguang Li
AU - Zhanyang Lin
AU - Mingrui Du
AU - Xupei Yao
AU - Shiming Liu
AU - Shiao Chen
AU - Haijian Su
AU - Liang Chen
AU - Yanke Shi
PY - 2026
DA - 2026/11/12
JO - Polymers
DO - 10.3390/polym18222828
UR - https://www.mdpi.com/2073-4360/18/22/2828
AB - Invert voids beneath underground concrete pipelines can cause support loss and settlement, while the spatial evolution of interfacial forces generated by confined polymer foaming remains poorly understood. Small-scale curved-interface grouting tests were conducted to investigate the effects of grout density, interface arch height, and circumferential position on local expansion forces, and a quadratic response surface model was developed for force prediction. Full-scale pipeline lifting tests were subsequently performed to investigate the relationship between interfacial expansion and structural displacement. The expansion response exhibited three stages—filling, rapid foaming, and stabilization—with pronounced spatial nonuniformity. Increasing grout density from 0.26 to 0.36 g/cm3 increased the peak expansion force by 58.9–69.7%, whereas increasing arch height from 8.14 to 14.60 mm resulted in an increase of only 5.3–9.2%. The response surface model showed good agreement with the experimental data used for model development (R2 = 0.9896). The full-scale test achieved a pipeline uplift of 50 mm, with the bell section lifting approximately 2.1 times faster than the spigot section during rapid uplift. A simplified equilibrium analysis yielded a theoretical critical grout density of 0.29 g/cm3 for initiating pipe uplift providing a preliminary reference for grouting parameter design and pipeline rehabilitation.