From Waste to Ship Materials: Development and Performance of Recycled Polymer Composites for Sustainable Maritime Applications
4 affiliations
- 1Department of Maritime Transportation and Management Engineering, Maritime Faculty, Kocaeli University, Kocaeli 41500, Türkiye
- 2Department of Maritime Busineess Management, Maritime Faculty, Kocaeli University, Kocaeli 41500, Türkiye
- 3Department of Polymer Materials Engineering, Faculty of Engineering, Yalova University, Yalova 77200, Türkiye
- 4Zamia Composite Research and Development Technology Joint Stock Company, ULUTEK Technopark, Nilüfer 16110, Türkiye
Abstract
This study investigates the potential of cone powder (PCP) as a sustainable filler in recycled polypropylene (rPP) composites for marine-related applications. Composites containing 5–20 wt.% PCP were manufactured by twin-screw extrusion and injection molding and characterized in terms of mechanical, thermal, chemical, morphological, and seawater absorption properties. At 20 wt.% PCP, flexural modulus and strength increased by 49.4% and 38.7%, respectively, compared with unfilled rPP. Tensile strength increased from 15.65 to 16.63 MPa, whereas impact strength decreased by 59.2% and elongation at break declined from 93.9% to 19.5%, indicating a stiffness–toughness trade-off. FTIR analysis identified characteristic lignocellulosic functional groups, while DSC revealed distinct melting transitions. TGA showed variations in initial degradation behavior, with principal degradation peaks remaining between 482.8 and 485.0 °C. After 960 h (40 days) of natural seawater immersion, absorption increased from 0.2005% for unfilled rPP to 1.1356% for the 20 wt.% PCP composite. Overall, PCP-containing rPP composites exhibited improved flexural performance but reduced impact resistance and increased moisture uptake. These findings suggest potential applications in selected marine-related components where stiffness is prioritized, although long-term durability and mechanical property retention after seawater exposure require further investigation.
Related
- Development and multi-response optimization of sustainable hemp fibre/cassia gum reinforced polyester hybrid composites for structural and insulation applications
- Development and optimization of sustainable sisal fibre/karaya gum reinforced polyester composites: Mechanical, thermal, dielectric and moisture absorption performance
- Development of high-performance sustainable epoxy bio-composites reinforced with banana fibre and marine shell-derived calcium carbonate filler
- SUSTAINABLE COMPOSITE MATERIALS FOR ELECTRIC VEHICLE APPLICATIONS: A COMPREHENSIVE REVIEW
- Optimization of multifunctional mechanical, thermo-mechanical, dielectric, and moisture resistance properties of Margosa gum reinforced epoxy composites for sustainable engineering applications
BibTeX
@article{sengul2026from,
title = {{From Waste to Ship Materials: Development and Performance of Recycled Polymer Composites for Sustainable Maritime Applications}},
author = {Ömer Şengül and Murat Yorulmaz and İdris Karagöz},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18232945},
url = {https://www.mdpi.com/2073-4360/18/23/2945},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - From Waste to Ship Materials: Development and Performance of Recycled Polymer Composites for Sustainable Maritime Applications
AU - Ömer Şengül
AU - Murat Yorulmaz
AU - İdris Karagöz
PY - 2026
DA - 2026/11/24
JO - Polymers
DO - 10.3390/polym18232945
UR - https://www.mdpi.com/2073-4360/18/23/2945
AB - This study investigates the potential of cone powder (PCP) as a sustainable filler in recycled polypropylene (rPP) composites for marine-related applications. Composites containing 5–20 wt.% PCP were manufactured by twin-screw extrusion and injection molding and characterized in terms of mechanical, thermal, chemical, morphological, and seawater absorption properties. At 20 wt.% PCP, flexural modulus and strength increased by 49.4% and 38.7%, respectively, compared with unfilled rPP. Tensile strength increased from 15.65 to 16.63 MPa, whereas impact strength decreased by 59.2% and elongation at break declined from 93.9% to 19.5%, indicating a stiffness–toughness trade-off. FTIR analysis identified characteristic lignocellulosic functional groups, while DSC revealed distinct melting transitions. TGA showed variations in initial degradation behavior, with principal degradation peaks remaining between 482.8 and 485.0 °C. After 960 h (40 days) of natural seawater immersion, absorption increased from 0.2005% for unfilled rPP to 1.1356% for the 20 wt.% PCP composite. Overall, PCP-containing rPP composites exhibited improved flexural performance but reduced impact resistance and increased moisture uptake. These findings suggest potential applications in selected marine-related components where stiffness is prioritized, although long-term durability and mechanical property retention after seawater exposure require further investigation.
SN - 2073-4360
ER -