Effect of Hexagonal Boron Nitride Nanoparticles on the Push-Out Bond Strength of a Bioceramic Root Canal Sealer

  1. 1Department of Endodontics, Faculty of Dentistry, University of Istanbul Medeniyet, Istanbul 34956, Türkiye

Abstract

This in vitro study evaluated the effect of hexagonal boron nitride (HBN) nanoparticles on the push-out bond strength of a bioceramic root canal sealer. Sixty-eight extracted human maxillary central incisors were prepared using Reciproc R40 instruments and assigned to four groups: Adseal, unmodified BioRoot RCS, and BioRoot RCS containing 5% or 20% HBN by volume. Following obturation with gutta-percha and the respective sealers, specimens were stored at 37 °C and 100% humidity for 14 days. One-millimeter-thick slices from the coronal, middle, and apical thirds underwent push-out testing. Data were analyzed using a linear mixed-effects model, with sealer type, root region, and their interaction as fixed effects and tooth identity as a random effect (p < 0.05). BioRoot RCS containing 20% HBN showed significantly higher bond strength than Adseal in the coronal region, no significant difference in the middle region, and significantly lower bond strength in the apical region. Unmodified BioRoot RCS showed the lowest bond strength in all regions. Regional variations differed according to sealer type. Within the limitations of this study, incorporating 20% HBN increased the push-out bond strength of BioRoot RCS. Further investigation of the physicochemical, biological, and long-term properties of HBN-modified sealers is required.

Related

  1. Effect of Hexagonal Boron Nitride (h-BN) Content on the Mechanical and Tribological Properties of Fused Deposition Modeling (FDM)-Printed PETG Composites
    PolymersPeer-reviewedCC BYFull textMaterials & polymersEurope PMC
  2. Mechanosensitive ion transport in hexagonal boron nitride nanopores
    Mohit Saraswat, Yechan Noh, Alex T. Hall +10
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  3. Nonradiative energy transfer between boron vacancies in hexagonal boron nitride and other two-dimensional materials
    Jules Fraunié, Mikhail Glazov, Sébastien Roux +14
    Physical Review BPeer-reviewedLicence not statedMaterials & polymersHAL
  4. Aromatic Molecular Emitters in a Hexagonal Boron Nitride Stack.
    Tianyu Fang, Ricardo Gioia Alvarez, Babak Behjati +8
    Nano lettersPeer-reviewedCC BYFull textMaterials & polymersEurope PMC
  5. Facile Etching Process for the Porous Structure of Hexagonal Boron Nitride as a Catalyst Support Using Metal Oxides Under Low-Temperature Conditions
    Myeung-Jin Lee, Donghyeok Kim, Nahea Kim +5
    CatalystsPeer-reviewedCC BY 4.0Materials & polymersCrossref
BibTeX
@article{ozkocak2026effect,
  title = {{Effect of Hexagonal Boron Nitride Nanoparticles on the Push-Out Bond Strength of a Bioceramic Root Canal Sealer}},
  author = {Ismail Ozkocak and Ikbal Sena Celebi Keskin and Banu Arıcıoglu},
  journal = {Nanomaterials},
  year = {2026},
  month = nov,
  doi = {10.3390/nano16211447},
  url = {https://www.mdpi.com/2079-4991/16/21/1447},
  note = {CC BY 4.0},
}
RIS
TY  - JOUR
TI  - Effect of Hexagonal Boron Nitride Nanoparticles on the Push-Out Bond Strength of a Bioceramic Root Canal Sealer
AU  - Ismail Ozkocak
AU  - Ikbal Sena Celebi Keskin
AU  - Banu Arıcıoglu
PY  - 2026
DA  - 2026/11/08
JO  - Nanomaterials
DO  - 10.3390/nano16211447
UR  - https://www.mdpi.com/2079-4991/16/21/1447
AB  - This in vitro study evaluated the effect of hexagonal boron nitride (HBN) nanoparticles on the push-out bond strength of a bioceramic root canal sealer. Sixty-eight extracted human maxillary central incisors were prepared using Reciproc R40 instruments and assigned to four groups: Adseal, unmodified BioRoot RCS, and BioRoot RCS containing 5% or 20% HBN by volume. Following obturation with gutta-percha and the respective sealers, specimens were stored at 37 °C and 100% humidity for 14 days. One-millimeter-thick slices from the coronal, middle, and apical thirds underwent push-out testing. Data were analyzed using a linear mixed-effects model, with sealer type, root region, and their interaction as fixed effects and tooth identity as a random effect (p < 0.05). BioRoot RCS containing 20% HBN showed significantly higher bond strength than Adseal in the coronal region, no significant difference in the middle region, and significantly lower bond strength in the apical region. Unmodified BioRoot RCS showed the lowest bond strength in all regions. Regional variations differed according to sealer type. Within the limitations of this study, incorporating 20% HBN increased the push-out bond strength of BioRoot RCS. Further investigation of the physicochemical, biological, and long-term properties of HBN-modified sealers is required.
SN  - 2079-4991
ER  -