Passive Self-Heating Is a Natural Equalizer: Quantitative Characterization, Capability Boundaries, and the Gain Surface of Consistency Flattening in Series Sodium-Ion Battery Packs

Abstract

Problem. Cell-to-cell internal-resistance dispersion is amplified at sub-zero temperatures and is widely regarded as the root cause of pack-level capacity loss and lifetime divergence. Industry and academia converge on one idea: eliminate the dispersion—active balancing, external preheating, and stringent dual-parameter sorting. A reversed proposition has been largely overlooked: in a series string, where current is common, resistance dispersion itself drives a passive self-homogenization mechanism—the highest-resistance cell dissipates the most Joule heat, warms the most, and its resistance drops the most, so it “catches up” with its lower-resistance neighbours. Ref. [1] proved that the sign of this compression is locked solely by 𝜕R/𝜕T<0. This paper answers the follow-up questions: how much? when does it fail? is it stable in the long run? can a quantitative surface be provided to guide sorting? Contributions. Using a physics-based sandbox calibrated against published measurements (second-order RC + VTF viscosity + Arrhenius coupling + lumped thermal model including entropic heat + concentrationpolarization truncation + dual capacity/resistance dispersion), we report six results: 1. First systematic quantification: at −30 °C/0.5C the capacity COV is flattened by 39.7% (3.47%→2.09%) with mean capacity +9.9%; the high-resistance group’s capacity rises +12.2% versus +8.0% for the low-resistance group, narrowing the high–low gap by 33.9%. Results are consistent before and after completing the physical model (40.7%→39.7%), excluding a modeling artifact. 2. Capability boundary: the mechanism is a resistance corrector, not a capacity corrector—it fails (and even mildly reverses) once capacity COV reaches about 3%; yet even when flattening is marginal, mean usable capacity still rises by about 5%. 3. C-rate sweet spot: a narrow window of 0.5–0.8C with threshold activation rather than gradual enhancement (a 12.7 pp jump from 0.45C to 0.5C); at 0.8C the flattening reaches 92.4% (isothermal COV 31.7% versus thermal 2.4%) and usable capacity is recovered by a factor of 5.5; at 1.0C everything is extinguished. 4. Full-temperature applicability domain: short-term flattening decreases monotonically from 69.4% at −30 °C to zero at 40 °C—it is a low-temperature-specific tool; at room temperature cells are already highly consistent and need no flattening. 5. Long-term stability: after 500 cycles the COV has not widened at all (both groups 4.46%)—the negative feedback exactly offsets the aging positive feedback of the central cells (aging-rate ratio 1.27×). Entropy generation—the industry’s universal villain—turns out to be a benefactor in lowtemperature self-heating. 6. Gain surface 𝜂=f(COV_Q,COV_R): capacity COVcontributes 69.1%of the variance (dominant) and resistance COV 30.9%; a threefold change in resistance COV perturbs the residual COV by ≤0.06 pp—resistance dispersion is “eaten clean” by self-heating, and the residual floor is set by capacity.

Related

  1. Structural–Response Consistency Evaluation of a Jiulong Coking Coal Molecular Model Based on Multi-Characterization Constraints
    Yanming Wang, Baoshan Jia, Zhihao Fu +2
    ACS OmegaPeer-reviewedCC BY-NC-ND 4.0Full textGeneral chemistryCrossref
  2. Quantitative Cryogenic Orbitrap Secondary Ion Mass Spectrometry for structural characterization of lipid nanoparticles
    Joseph W Roberts, Anna Kotowska, Eduardo Aguilar-Bejarano +13
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  3. Quantitative Characterization of Pharmaceutical Powder Surface Interactions Using Inverse Gas Chromatography-Derived Surface Energy Profiles
    Ken Yoshioka, Kohei Tahara
    ChemRxivPreprintCC BYFull textPhysical chemistryChemRxiv
  4. Effect of Low-Frequency Pulsating Water Injection Parameters on Coal Permeability: Quantitative Characterization Experiments and a Field Case Study
    Huijing Fang, Ang Xu, Hai Ding +3
    ACS OmegaPeer-reviewedCC BY-NC-ND 4.0Full textGeneral chemistryCrossrefPMC
  5. Quantitative characterization of flow regimes in Continuous Oscillatory Baffled Reactors using PIV and POD analysis
    Rita Branco, Margarida S.C.A. Brito, Martine Poux +1
    Chemical Engineering SciencePeer-reviewedCC BY-NC-ND 4.0Full textGeneral chemistryHAL
BibTeX
@misc{yang2026passive,
  title = {{Passive Self-Heating Is a Natural Equalizer: Quantitative Characterization, Capability Boundaries, and the Gain Surface of Consistency Flattening in Series Sodium-Ion Battery Packs}},
  author = {Bo Yang and 杨博 杨},
  howpublished = {ChemRxiv},
  year = {2026},
  month = oct,
  doi = {10.26434/chemrxiv.15011108/v1},
  url = {https://chemrxiv.org/doi/full/10.26434/chemrxiv.15011108/v1},
  note = {CC BY},
}
RIS
TY  - UNPB
TI  - Passive Self-Heating Is a Natural Equalizer: Quantitative Characterization, Capability Boundaries, and the Gain Surface of Consistency Flattening in Series Sodium-Ion Battery Packs
AU  - Bo Yang
AU  - 杨博 杨
PY  - 2026
DA  - 2026/10/27
PB  - ChemRxiv
DO  - 10.26434/chemrxiv.15011108/v1
UR  - https://chemrxiv.org/doi/full/10.26434/chemrxiv.15011108/v1
AB  - Problem. Cell-to-cell internal-resistance dispersion is amplified at sub-zero temperatures and is widely regarded as the root cause of pack-level capacity loss and lifetime divergence. Industry and academia converge on one idea: eliminate the dispersion—active balancing, external preheating, and stringent dual-parameter sorting. A reversed proposition has been largely overlooked: in a series string, where current is common, resistance dispersion itself drives a passive self-homogenization mechanism—the highest-resistance cell dissipates the most Joule heat, warms the most, and its resistance drops the most, so it “catches up” with its lower-resistance neighbours. Ref. [1] proved that the sign of this compression is locked solely by 𝜕R/𝜕T<0. This paper answers the follow-up questions: how much? when does it fail? is it stable in the long run? can a quantitative surface be provided to guide sorting? Contributions. Using a physics-based sandbox calibrated against published measurements (second-order RC + VTF viscosity + Arrhenius coupling + lumped thermal model including entropic heat + concentrationpolarization truncation + dual capacity/resistance dispersion), we report six results: 1. First systematic quantification: at −30 °C/0.5C the capacity COV is flattened by 39.7% (3.47%→2.09%) with mean capacity +9.9%; the high-resistance group’s capacity rises +12.2% versus +8.0% for the low-resistance group, narrowing the high–low gap by 33.9%. Results are consistent before and after completing the physical model (40.7%→39.7%), excluding a modeling artifact. 2. Capability boundary: the mechanism is a resistance corrector, not a capacity corrector—it fails (and even mildly reverses) once capacity COV reaches about 3%; yet even when flattening is marginal, mean usable capacity still rises by about 5%. 3. C-rate sweet spot: a narrow window of 0.5–0.8C with threshold activation rather than gradual enhancement (a 12.7 pp jump from 0.45C to 0.5C); at 0.8C the flattening reaches 92.4% (isothermal COV 31.7% versus thermal 2.4%) and usable capacity is recovered by a factor of 5.5; at 1.0C everything is extinguished. 4. Full-temperature applicability domain: short-term flattening decreases monotonically from 69.4% at −30 °C to zero at 40 °C—it is a low-temperature-specific tool; at room temperature cells are already highly consistent and need no flattening. 5. Long-term stability: after 500 cycles the COV has not widened at all (both groups 4.46%)—the negative feedback exactly offsets the aging positive feedback of the central cells (aging-rate ratio 1.27×). Entropy generation—the industry’s universal villain—turns out to be a benefactor in lowtemperature self-heating. 6. Gain surface 𝜂=f(COV_Q,COV_R): capacity COVcontributes 69.1%of the variance (dominant) and resistance COV 30.9%; a threefold change in resistance COV perturbs the residual COV by ≤0.06 pp—resistance dispersion is “eaten clean” by self-heating, and the residual floor is set by capacity.
ER  -