Atomistic insights into hydrogen diffusion mechanisms, multi-step dehydrogenation, and strain-engineered thermodynamics in orthorhombic ternary magnesium hydrides.

5 affiliations
  1. 1Physico-chemistry of Materials Team, Abdelmalek Essaâdi University of Tetouan, Faculty of Sciences Morocco [email protected].
  2. 2Radiations and Nuclear Systems Group, FS, Abdelmalek Essaadi University Tetouan Morocco.
  3. 3Optics, Materials and Systems Team, Faculty of Sciences, Abdelmalek Essaâdi University Tetouan Morocco.
  4. 4Materials and Interfacial Systems Laboratory, Abdelmalek Essaâdi University, Faculty of Sciences Tetouan Morocco.
  5. 5Materials, Membranes and Nanotechnology Research Team, Moulay Ismail University of Meknès, Faculty of Sciences BP: 11201 Zitoune Meknès Morocco.

Abstract

Solid-state complex hydrides offer a promising solution for safe hydrogen storage, yet practical applications remain constrained by high thermodynamic stability and sluggish kinetics. In this study, orthorhombic strontium magnesium tetrahydride (SrMgH₄, space group Cmc2₁) was investigated using Density Functional Theory (DFT). SrMgH₄ exhibits mechanical stability via Born criteria, dynamic lattice stability from phonon dispersion, and a wide bandgap of E g = 2.836 eV (3.801 eV via the HSE06 hybrid functional). It delivers a theoretical gravimetric capacity of 3.48 wt% and an outstanding volumetric density of 88.18 g H₂ per L. From a kinetic perspective, the LST/QST method predicts that SrMgH₄ has fast diffusion pathways with energy barriers as low as 0.242 eV along the H₃-H₄ path, and an interconnected 3D percolating network (≤0.482 eV). It is predicted that the single-step decomposition of SrMgH₄ would require a desorption temperature of 768 K in its undeformed state. However, an intermediate pathway via the binary compound SrH₂ significantly lowers the desorption temperature to 546 K. Additionally, applying a triaxial strain of -4% to -5% lowers the desorption temperature to 345.0 K, making it within the goals of the US Department of Energy (DOE). These results indicate that SrMgH4 is an excellent material for reversible solid state hydrogen storage.

Related

  1. Atomistic mechanisms of hard carbon formation from polyvinylidene chloride.
    Litong Wu, Zitong Wu, Zakariya El-Machachi +1
    Chemical sciencePeer-reviewedCC BYFull textOrganic chemistryEurope PMCPMC
  2. Orthorhombic crystal structured Dy3+ doped Li2Cd2(PO4)2 nanopowders for yellowish light emitting solid state lighting applications
    Shaik Azad Basha, K. Srinivasarao, K. Daniel +3
    Chemical PapersPeer-reviewedLicence not statedFull text7 citedMaterials & polymersOpenAlex
  3. (De)Sodiation Mechanisms and Cycling Stability of Entropy‐Engineered Sodium‐Ion Battery Alloy Anodes by Operando X‐ray Diffraction
    Kuray Dericiler, Sajid Alvi, Amanda Persdotter +5
    Batteries & SupercapsPeer-reviewedCC BY 4.0Full textMaterials & polymersHAL
  4. Engineered carbon-based fertilizers for sustainable agriculture: physicochemical mechanisms of nutrient release, soil health improvement, and plant uptake
    Othman Al-Dossary, Tauqeer Ahmed Qadri, Rashid Abbas Khan +5
    RSC AdvancesPeer-reviewedCC BY 3.0Full textGeneral chemistryPMC
  5. Exsolution-Engineered Ni-Based Titanate Perovskites for Dry Reforming of Methane: Activity-Stability Trade-Offs and Deactivation Mechanisms
    Jonathan Cavazzani, Andrea Osti, Lorenzo Rizzato +2
    ACS OmegaPeer-reviewedCC BY 4.0Full textCatalysisCrossrefPMC
BibTeX
@article{arfoy2026atomistic,
  title = {{Atomistic insights into hydrogen diffusion mechanisms, multi-step dehydrogenation, and strain-engineered thermodynamics in orthorhombic ternary magnesium hydrides.}},
  author = {Brahim Arfoy and Mohamed Drissi El-Bouzaidi and Oualid Elhaddade and Mohammed Es-Saddik and Abdelhadi El Hachmi and Leila Loubbidi and Khalid Draoui and Mohamed Douma and ElHossain Chtoun},
  journal = {RSC advances},
  year = {2026},
  month = nov,
  doi = {10.1039/d6ra10283b},
  url = {https://europepmc.org/article/MED/43061208},
  note = {CC BY},
}
RIS
TY  - JOUR
TI  - Atomistic insights into hydrogen diffusion mechanisms, multi-step dehydrogenation, and strain-engineered thermodynamics in orthorhombic ternary magnesium hydrides.
AU  - Brahim Arfoy
AU  - Mohamed Drissi El-Bouzaidi
AU  - Oualid Elhaddade
AU  - Mohammed Es-Saddik
AU  - Abdelhadi El Hachmi
AU  - Leila Loubbidi
AU  - Khalid Draoui
AU  - Mohamed Douma
AU  - ElHossain Chtoun
PY  - 2026
DA  - 2026/11/19
JO  - RSC advances
DO  - 10.1039/d6ra10283b
UR  - https://europepmc.org/article/MED/43061208
AB  - Solid-state complex hydrides offer a promising solution for safe hydrogen storage, yet practical applications remain constrained by high thermodynamic stability and sluggish kinetics. In this study, orthorhombic strontium magnesium tetrahydride (SrMgH₄, space group Cmc2₁) was investigated using Density Functional Theory (DFT). SrMgH₄ exhibits mechanical stability via Born criteria, dynamic lattice stability from phonon dispersion, and a wide bandgap of E g = 2.836 eV (3.801 eV via the HSE06 hybrid functional). It delivers a theoretical gravimetric capacity of 3.48 wt% and an outstanding volumetric density of 88.18 g H₂ per L. From a kinetic perspective, the LST/QST method predicts that SrMgH₄ has fast diffusion pathways with energy barriers as low as 0.242 eV along the H₃-H₄ path, and an interconnected 3D percolating network (≤0.482 eV). It is predicted that the single-step decomposition of SrMgH₄ would require a desorption temperature of 768 K in its undeformed state. However, an intermediate pathway via the binary compound SrH₂ significantly lowers the desorption temperature to 546 K. Additionally, applying a triaxial strain of -4% to -5% lowers the desorption temperature to 345.0 K, making it within the goals of the US Department of Energy (DOE). These results indicate that SrMgH4 is an excellent material for reversible solid state hydrogen storage.
SN  - 2046-2069
ER  -