Skip to content
DraconiticResearch
Search Sources API
194,161 studies31 sourcesUpdated 40 min ago
Peer-reviewedCC BY-NC-NDACS omega

The Effect of Coke Powder on the Iron Ore Fines Reduction by Carbon Monoxide

  1. 1Shandong University , , , ,
  2. 2King’s College London , , Strand , ,
  3. 3Shanxi Research Institute of Huairou Laboratory , , ,

Abstract

Iron ore fines and coke powder are synergistically reduced in a drop-tube reactor. The effects of temperature, CO concentration, and the blending ratio (BR) of coke powder are investigated. The results show that increasing temperature promotes reduction within the range of 800–1200 °C, while CO concentration has a lesser effect. The kinetic mechanism can be explained by a nucleation-and-growth model, and the activation energies for iron ore fines, the mixture with fine coke powder at BR = 0.4, and the mixture with the same particle size coke powder at BR = 0.4 are 19.09 kJ/mol, 50.61 kJ/mol, and 47.80 kJ/mol, respectively. Coke powder causes the outlet CO concentration to be equal to or greater than the inlet CO concentration and the outlet CO2 concentration decreases. Increasing BR from 0.4 to 0.8 and 0.8 to 1.2 mainly promoted the conversion of Fe3O4→FeO and FeO→Fe, respectively. The sticking index reached a minimum of 0.86% when BR = 0.4. However, overall sticking inhibition was more effective when BR = 1.2. The mechanism of sticking inhibition is that the coke powder acts as a physical barrier, reducing the collision and contact probability between the iron ore fines, thereby preventing iron whiskers from entangling or bridging.

Related

  1. O2-tolerant CO2-to-CO reduction by air-sensitive carbon monoxide dehydrogenases in hydrated deep eutectic solvents
    Léonard Olivotto, Claudio Righetti, Julien Pérard +3
    EES CatalysisPeer-reviewedCC BY 4.0Full textCatalysisMaterials & polymersHAL
  2. Analysis and Modeling of Iron Ore Reduction and Melting Behavior under Blast Furnace Ore-Coke Coupling Conditions
    Mingxin Wu, Jinbo Li, Tingle Li +4
    ACS OmegaPeer-reviewedCC BY-NC-ND 4.0Full textGeneral chemistryCrossrefEurope PMC
  3. Short-Rotation Coppice Pellets as Biofuels in a Modern Boiler with an Electrostatic Precipitator: Particulate Matter and Carbon Monoxide Emissions
    Kazimierz Warmiński, Paweł Dudziec, Adam Nocoń +1
    Molecules (Basel, Switzerland)Peer-reviewedCC BYFull textGeneral chemistryEurope PMC
  4. Tuning covalence for phosphorus-mediated C-C coupling in carbon monoxide electroreduction to multicarbon oxygenates
    Anissa Ghoridi, Carlos V. M. Inocêncio, Hong Phong Duong +19
    ChemRxivPreprintCC BYGeneral chemistryChemRxiv
  5. Physics-Guided Concentration Inference from Resistance Transients in a Mixed-Phase SnO-SnO2 Carbon Monoxide Sensor with p-n Switching
    Sani Biswas, Preetam Singh, Amit Kumar Gangwar
    arXivPreprintarXiv licenceFull textPhysical chemistryApplied physics & instrumentationarXiv
BibTeX
@article{zhao2026effect,
  title = {{The Effect of Coke Powder on the Iron Ore Fines Reduction by Carbon Monoxide}},
  author = {Yuan Zhao and Tao Wang and Tianming Xu and Binxuan Zhou and Yong Dong and Chunyuan Ma},
  journal = {ACS omega},
  year = {2026},
  month = oct,
  doi = {10.1021/acsomega.6c05900},
  url = {https://europepmc.org/article/PMC/PMC13670866},
  note = {CC BY-NC-ND},
}
RIS
TY  - JOUR
TI  - The Effect of Coke Powder on the Iron Ore Fines Reduction by Carbon Monoxide
AU  - Yuan Zhao
AU  - Tao Wang
AU  - Tianming Xu
AU  - Binxuan Zhou
AU  - Yong Dong
AU  - Chunyuan Ma
PY  - 2026
DA  - 2026/10/01
JO  - ACS omega
DO  - 10.1021/acsomega.6c05900
UR  - https://europepmc.org/article/PMC/PMC13670866
AB  - Iron ore fines and coke powder are synergistically reduced in a drop-tube reactor. The effects of temperature, CO concentration, and the blending ratio (BR) of coke powder are investigated. The results show that increasing temperature promotes reduction within the range of 800–1200 °C, while CO concentration has a lesser effect. The kinetic mechanism can be explained by a nucleation-and-growth model, and the activation energies for iron ore fines, the mixture with fine coke powder at BR = 0.4, and the mixture with the same particle size coke powder at BR = 0.4 are 19.09 kJ/mol, 50.61 kJ/mol, and 47.80 kJ/mol, respectively. Coke powder causes the outlet CO concentration to be equal to or greater than the inlet CO concentration and the outlet CO2 concentration decreases. Increasing BR from 0.4 to 0.8 and 0.8 to 1.2 mainly promoted the conversion of Fe3O4→FeO and FeO→Fe, respectively. The sticking index reached a minimum of 0.86% when BR = 0.4. However, overall sticking inhibition was more effective when BR = 1.2. The mechanism of sticking inhibition is that the coke powder acts as a physical barrier, reducing the collision and contact probability between the iron ore fines, thereby preventing iron whiskers from entangling or bridging.
SN  - 2470-1343
ER  -