Skip to content
DraconiticResearch
Search Sources API
197,768 studies31 sourcesUpdated 26 min ago
PreprintCC BYChemRxiv

Molecular Hydrogen Governs Zinc-Based Battery Failure

  1. 1Chimie du solide et de l’Energie, UMR 8260, Collège de France
  2. 2Réseau sur le stockage Electrochimique de l’Energie (RS2E
  3. 3Université Paris Cité, ITODYS, CNRS, 15 Rue Jean Antoine de Baïf, Paris, France, 75013

Abstract

Zinc is among the most promising anode materials for sustainable aqueous batteries, yet its practical deployment is limited by poor interfacial stability and insufficient durability. Because the thermodynamic stability of zinc is incompatible with the water stability window, corrosion and hydrogen evolution inevitably accompany zinc electrochemistry in aqueous electrolytes. Despite being an inherent product of zinc corrosion, molecular hydrogen (H2) has largely been regarded as a passive by-product rather than an active contributor to zinc degradation and dendrite formation. Here, we demonstrate that H2 directly governs zinc deposition and stripping across multiple length scales. By combining operando fibre-optic surface plasmon resonance, electrochemical quartz crystal microbalance, X-ray diffraction and operando optical microscopy, we resolve the influence of H2 on the zinc–electrolyte interface from interfacial processes to macroscopic deposit growth. Dissolved H2 destabilizes zinc electrodeposition by increasing the plating overpotential and altering deposition dynamics. It induces a crystallographic texture transition from the basal (002) to the prismatic (101) orientation, producing more porous deposits and modifying the growth kinetics of the zinc deposition front. Quantitative optical-flow analysis further reveals that H2 accelerates local growth dynamics and increases interfacial roughness, thereby compromising deposition uniformity. These effects persist across different electrolyte chemistries and current densities, establishing molecular hydrogen as an active regulator of zinc interfacial stability. Consequently, H2 reduces the cycling lifetime of zinc symmetric cells and promotes premature short circuits in Zn–MnO2 batteries. These findings identify molecular hydrogen as a previously overlooked driver of the morphological and crystallographic evolution of zinc deposits and establish hydrogen management as a design principle for stabilizing the zinc–electrolyte interface. Controlling dissolved H2, including through electrolyte degassing strategies, therefore provides a route towards suppressing dendritic growth, extending battery lifetime and enabling more durable aqueous zinc batteries.

Related

  1. Asymmetric Zinc-Nitrate/Hydrogen Battery Chemistry Coupling Electrochemical Hydrogen Charge and Energy Storage.
    Zhijie Yan, Xinrong Chen, Chunpeng Yang
    JACS AuPeer-reviewedCC BY-NC-NDFull textGeneral chemistryEurope PMCPMC
  2. Matrix Confinement Governs Competing Heavy‑Atom and Hydrogen Tunneling Pathways
    Heng-Ding Wang, Hao Wu, Yu-Wei Yan +6
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  3. Powering Hyperscale AI Data Centers with Off-grid Solar, Battery, and Hydrogen
    Anil Bika, Brian Setzler, Paul Browning +6
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  4. Hydrogen‐Bond Enabled Phosphite Based Intrinsic Flame‐Retardant Solid‐Solid Phase Change Materials Using Catalyst/Solvent‐Free Multi‐Component Reaction for Battery Thermal Management
    Changhui Liu, Guangyuan Liang, Yuanzheng Liu +7
    Advanced SciencePeer-reviewedCC BY 4.0Full text1 citedMaterials & polymersPMC
  5. Charged Interface in Battery Breaks Molecular Chiral Symmetry
    Chao Chen, Dengpan Dong, Yanjin Liu +8
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
BibTeX
@misc{chotard2026molecular,
  title = {{Molecular Hydrogen Governs Zinc-Based Battery Failure}},
  author = {Hugo Chotard and Murugasenapathi N K and Özlem Sel and Frédéric Kanoufi and Jean-Marie Tarascon and Ivette Aguilar},
  howpublished = {ChemRxiv},
  year = {2026},
  month = sep,
  doi = {10.26434/chemrxiv.15008306/v1},
  url = {https://chemrxiv.org/doi/full/10.26434/chemrxiv.15008306/v1},
  note = {CC BY},
}
RIS
TY  - UNPB
TI  - Molecular Hydrogen Governs Zinc-Based Battery Failure
AU  - Hugo Chotard
AU  - Murugasenapathi N K
AU  - Özlem Sel
AU  - Frédéric Kanoufi
AU  - Jean-Marie Tarascon
AU  - Ivette Aguilar
PY  - 2026
DA  - 2026/09/04
PB  - ChemRxiv
DO  - 10.26434/chemrxiv.15008306/v1
UR  - https://chemrxiv.org/doi/full/10.26434/chemrxiv.15008306/v1
AB  - Zinc is among the most promising anode materials for sustainable aqueous batteries, yet its practical deployment is limited by poor interfacial stability and insufficient durability. Because the thermodynamic stability of zinc is incompatible with the water stability window, corrosion and hydrogen evolution inevitably accompany zinc electrochemistry in aqueous electrolytes. Despite being an inherent product of zinc corrosion, molecular hydrogen (H2) has largely been regarded as a passive by-product rather than an active contributor to zinc degradation and dendrite formation. Here, we demonstrate that H2 directly governs zinc deposition and stripping across multiple length scales. By combining operando fibre-optic surface plasmon resonance, electrochemical quartz crystal microbalance, X-ray diffraction and operando optical microscopy, we resolve the influence of H2 on the zinc–electrolyte interface from interfacial processes to macroscopic deposit growth. Dissolved H2 destabilizes zinc electrodeposition by increasing the plating overpotential and altering deposition dynamics. It induces a crystallographic texture transition from the basal (002) to the prismatic (101) orientation, producing more porous deposits and modifying the growth kinetics of the zinc deposition front. Quantitative optical-flow analysis further reveals that H2 accelerates local growth dynamics and increases interfacial roughness, thereby compromising deposition uniformity. These effects persist across different electrolyte chemistries and current densities, establishing molecular hydrogen as an active regulator of zinc interfacial stability. Consequently, H2 reduces the cycling lifetime of zinc symmetric cells and promotes premature short circuits in Zn–MnO2 batteries. These findings identify molecular hydrogen as a previously overlooked driver of the morphological and crystallographic evolution of zinc deposits and establish hydrogen management as a design principle for stabilizing the zinc–electrolyte interface. Controlling dissolved H2, including through electrolyte degassing strategies, therefore provides a route towards suppressing dendritic growth, extending battery lifetime and enabling more durable aqueous zinc batteries.
ER  -