Stabilization of Acidic Uranium Tailings Residue Using a Cement-Fly Ash-Zero-Valent Iron Composite: Mechanical Performance and Long-Term Leaching Behavior.
- 1Beijing Research Institute of Chemical Engineering and Metallurgy, China National Nuclear Corporation, Beijing 101149, China.
- 2Zhonghe Mining Technology Co., Ltd., Beijing 100022, China.
Abstract
Acid-leached uranium tailings residues present a long-term management challenge because uranium mobility, sulfur-driven acidification, and poor structural stability must be controlled simultaneously. This study developed a multifunctional stabilization/solidification strategy combining Portland cement, fly ash (FA), and zero-valent iron (Fe⁰) for acidic uranium tailings residue generated after sulfuric-acid extraction. The residue contained approximately 0.011% U and high Si-Al and sulfur contents, and showed a marginal acid-base balance, with an acid-neutralization capacity of 83.3 and maximum potential acidity of 75.3. Fine particles exhibited higher porosity and greater uranium release. Cement-to-residue ratio, water-to-cement ratio, curing age, FA replacement, and Fe⁰ addition were systematically evaluated. A cement-to-residue ratio of 3:7 and water-to-cement ratio of 0.6 yielded a 28 d unconfined compressive strength of 28.7 MPa. Incorporation of 15-25% FA with 1% Fe⁰ maintained strength at approximately 30 MPa, while five freeze-thaw cycles caused only a 2.79% strength loss. Direct Fe⁰ treatment reduced cumulative uranium release by approximately 78%. Cement solidification maintained uranium concentrations below 10 μg L⁻¹ during 90 d leaching under acidic, neutral, and alkaline conditions, corresponding to >99% suppression relative to untreated residue, while cement + Fe⁰ further reduced uranium release to <1 μg L⁻¹. Sulfate release was reduced to less than one-third of that from untreated residue. Overall, cement, FA, and Fe⁰ provided complementary structural, matrix-modifying, and uranium-reactive functions, enabling simultaneous control of mechanical integrity and contaminant mobility.
Related
- Enhancement of thiourea leaching performance of refractory silver tailings by mechanical activation
- In vitro evaluation of the mechanical properties of the resin-based composite three-dimensional digital space maintainers containing glass ionomer cements as fluoride sources in pediatric dentistry
- Effects of keiser-assisted Nordic hamstring curl training on hamstring flexibility, mechanical properties, and pitching performance in high school baseball pitchers
- Performance and microstructural assessment of clay stabilization using ceramic siding waste powder and metakaolin-based geopolymer
- Performance evaluation and optimization of powder mixed EDM of Inconel 718 using composite electrodes and the VIKOR method
BibTeX
@article{niu2026stabilization,
title = {{Stabilization of Acidic Uranium Tailings Residue Using a Cement-Fly Ash-Zero-Valent Iron Composite: Mechanical Performance and Long-Term Leaching Behavior.}},
author = {Jie Niu and Yang Wang and Tongxin Duo and Dong Zhang and Mumtaz Khan and Xiaochao Liu and Dong Ji},
journal = {Toxics},
year = {2026},
month = oct,
doi = {10.3390/toxics14110950},
url = {https://europepmc.org/article/MED/43083560},
note = {CC BY},
}
RIS
TY - JOUR
TI - Stabilization of Acidic Uranium Tailings Residue Using a Cement-Fly Ash-Zero-Valent Iron Composite: Mechanical Performance and Long-Term Leaching Behavior.
AU - Jie Niu
AU - Yang Wang
AU - Tongxin Duo
AU - Dong Zhang
AU - Mumtaz Khan
AU - Xiaochao Liu
AU - Dong Ji
PY - 2026
DA - 2026/10/27
JO - Toxics
DO - 10.3390/toxics14110950
UR - https://europepmc.org/article/MED/43083560
AB - Acid-leached uranium tailings residues present a long-term management challenge because uranium mobility, sulfur-driven acidification, and poor structural stability must be controlled simultaneously. This study developed a multifunctional stabilization/solidification strategy combining Portland cement, fly ash (FA), and zero-valent iron (Fe⁰) for acidic uranium tailings residue generated after sulfuric-acid extraction. The residue contained approximately 0.011% U and high Si-Al and sulfur contents, and showed a marginal acid-base balance, with an acid-neutralization capacity of 83.3 and maximum potential acidity of 75.3. Fine particles exhibited higher porosity and greater uranium release. Cement-to-residue ratio, water-to-cement ratio, curing age, FA replacement, and Fe⁰ addition were systematically evaluated. A cement-to-residue ratio of 3:7 and water-to-cement ratio of 0.6 yielded a 28 d unconfined compressive strength of 28.7 MPa. Incorporation of 15-25% FA with 1% Fe⁰ maintained strength at approximately 30 MPa, while five freeze-thaw cycles caused only a 2.79% strength loss. Direct Fe⁰ treatment reduced cumulative uranium release by approximately 78%. Cement solidification maintained uranium concentrations below 10 μg L⁻¹ during 90 d leaching under acidic, neutral, and alkaline conditions, corresponding to >99% suppression relative to untreated residue, while cement + Fe⁰ further reduced uranium release to <1 μg L⁻¹. Sulfate release was reduced to less than one-third of that from untreated residue. Overall, cement, FA, and Fe⁰ provided complementary structural, matrix-modifying, and uranium-reactive functions, enabling simultaneous control of mechanical integrity and contaminant mobility.
SN - 2305-6304
ER -