Peer-reviewedCC BYRSC Advances
Synergistic effect of Mn substitution and ball milling on NaCu 0.2 Fe 0.8− x Mn x O 2 cathode materials for sodium-ion batteries
Abstract
= 0.7) did not show significant morphological changes in the electrode before and after cycling, confirming the high structural stability of our prepared electrodes during cycling.
Related
- Investigation of NaxFePO4 systems prepared by a modified Pechini sol-gel method as possible cathode materials for high voltage Na-ion batteries
- Surfactant incorporation enhancing the two-electron transfer reaction of MnO2 cathode materials in aqueous Zn batteries
- Thermal Runaway Characteristics of Batteries with Manganese-Based Composite Cathode Materials Triggered by Electromagnetic Induction Heating and Lateral Heating
- Enhancing ionic conductivity and interfacial stability of perovskite-type LLTO solid electrolytes via synergistic A-site Sr substitution and polymer layer engineering for safer lithium-ion batteries.
- Synthesis of Fused Biimidazole-Containing Polymers and Their Application as High-Potential Organic Cathode Materials for Lithium-Ion Batteries
BibTeX
@article{slima2026synergistic,
title = {{Synergistic effect of Mn substitution and ball milling on NaCu 0.2 Fe 0.8− x Mn x O 2 cathode materials for sodium-ion batteries}},
author = {Ichrak Ben Slima and Kawthar Trabelsi and Lahcen Fkhar and Karim Karoui and Frédéric Boschini and Abdallah Ben Rhaiem and Abdelfattah Mahmoud},
journal = {RSC Advances},
year = {2026},
month = jul,
doi = {10.1039/d6ra02392d},
url = {https://hal.science/hal-05752266v1},
note = {CC BY},
}
RIS
TY - JOUR
TI - Synergistic effect of Mn substitution and ball milling on NaCu 0.2 Fe 0.8− x Mn x O 2 cathode materials for sodium-ion batteries
AU - Ichrak Ben Slima
AU - Kawthar Trabelsi
AU - Lahcen Fkhar
AU - Karim Karoui
AU - Frédéric Boschini
AU - Abdallah Ben Rhaiem
AU - Abdelfattah Mahmoud
PY - 2026
DA - 2026/07/02
JO - RSC Advances
DO - 10.1039/d6ra02392d
UR - https://hal.science/hal-05752266v1
AB - = 0.7) did not show significant morphological changes in the electrode before and after cycling, confirming the high structural stability of our prepared electrodes during cycling.