Octadecylsilane-Functionalized Fe3O4 Nanoparticles Enhance Shape Fixity but Restrict Thermally Activated Shape Recovery in Thermoplastic Polyurethane Composites
- 1Tecnologico de Monterrey, School of Engineering and Sciences, Queretaro 76130, Mexico
- 2Tecnologico de Monterrey, Artificial Intelligence for Manufacturing and Supply Chain Institute, Queretaro 76130, Mexico
- 3Department of Industrial Technologies, Faculty of Engineering, Universidad de Talca, Curico 3340000, Chile
Abstract
Magnetite (Fe3O4) is often added to thermoplastic polyurethane (TPU) to fabricate thermally actuated shape memory parts, but the particles tend to agglomerate and interact poorly with the matrix. We prepared TPU composites with 10 wt% Fe3O4, either as received or coated with octadecyltrichlorosilane (ODTS), by tetrahydrofuran (THF) solution casting followed by micro-injection molding. Neat and THF-processed TPU were included as references so that the effects of solvent, filler and surface treatment could be separated. The 5% mass-loss temperature (T95%) was 314.2 °C for neat TPU and 309.7 °C for THF-processed TPU; bare Fe3O4 lowered it to 284.8 °C and ODTS-Fe3O4 to 292.3 °C. In differential scanning calorimetry (DSC), the ODTS composite kept the soft-segment glass transition at −21 °C, but its hard-segment crystallization and melting enthalpies fell by 72% and 74%. The stress at 150% strain (17.9–18.6 MPa) did not differ among formulations (ANOVA, p = 0.49), whereas bare Fe3O4 raised Young’s modulus from 0.106 to 0.125 GPa (p = 0.036). In angular shape memory tests with recovery triggered in an oven at 90 °C, the ODTS composite fixed the temporary shape best (shape fixity ratio/Rf = 91.9% against 86.4% for neat TPU) and recovered least after 240 s (11.0% against 47.1%). Across the four materials, recovery tracked the hard-domain melting enthalpy. We attribute the higher fixity and lower recovery primarily to the loss of physical netpoints; a contribution from particle–matrix interactions is possible but could not be separated with the present data. Magnetic actuation was not evaluated in this study. Silane treatments for magnetite-filled TPU should therefore be judged by their effect on hard-segment ordering as well as on dispersion.
Related
- Bidentate Click-Functionalized Thermoplastic Polyurethane for Modular Immobilization of PEGylated Compounds: Mirabegron as a Proof-of-Concept
- Mechanical performance and eco-efficiency of thermoplastic polyurethane composites reinforced with recycled tire rubber
- Deformation-Aware Monte Carlo Assessment of a Bi2O3/Thermoplastic Polyurethane Shielding Surrogate Under Tensile Strain and Local Thickness Loss
- Synthesis of PEDOT particles and manufacturing of electrically-conductive PEO / PEDOT thermoplastic composites by twin-screw extrusion
- Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers
BibTeX
@article{elias2026octadecylsilanefunctionalized,
title = {{Octadecylsilane-Functionalized Fe3O4 Nanoparticles Enhance Shape Fixity but Restrict Thermally Activated Shape Recovery in Thermoplastic Polyurethane Composites}},
author = {Abdiel Elias and Angel Anaya and F. I. Espinosa-Lagunes and Juan G. Sotelo and Gonzalo Pincheira-Orellana and Martin Sepulveda and Cecilia D. Treviño-Quintanilla},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18232950},
url = {https://www.mdpi.com/2073-4360/18/23/2950},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - Octadecylsilane-Functionalized Fe3O4 Nanoparticles Enhance Shape Fixity but Restrict Thermally Activated Shape Recovery in Thermoplastic Polyurethane Composites
AU - Abdiel Elias
AU - Angel Anaya
AU - F. I. Espinosa-Lagunes
AU - Juan G. Sotelo
AU - Gonzalo Pincheira-Orellana
AU - Martin Sepulveda
AU - Cecilia D. Treviño-Quintanilla
PY - 2026
DA - 2026/11/24
JO - Polymers
DO - 10.3390/polym18232950
UR - https://www.mdpi.com/2073-4360/18/23/2950
AB - Magnetite (Fe3O4) is often added to thermoplastic polyurethane (TPU) to fabricate thermally actuated shape memory parts, but the particles tend to agglomerate and interact poorly with the matrix. We prepared TPU composites with 10 wt% Fe3O4, either as received or coated with octadecyltrichlorosilane (ODTS), by tetrahydrofuran (THF) solution casting followed by micro-injection molding. Neat and THF-processed TPU were included as references so that the effects of solvent, filler and surface treatment could be separated. The 5% mass-loss temperature (T95%) was 314.2 °C for neat TPU and 309.7 °C for THF-processed TPU; bare Fe3O4 lowered it to 284.8 °C and ODTS-Fe3O4 to 292.3 °C. In differential scanning calorimetry (DSC), the ODTS composite kept the soft-segment glass transition at −21 °C, but its hard-segment crystallization and melting enthalpies fell by 72% and 74%. The stress at 150% strain (17.9–18.6 MPa) did not differ among formulations (ANOVA, p = 0.49), whereas bare Fe3O4 raised Young’s modulus from 0.106 to 0.125 GPa (p = 0.036). In angular shape memory tests with recovery triggered in an oven at 90 °C, the ODTS composite fixed the temporary shape best (shape fixity ratio/Rf = 91.9% against 86.4% for neat TPU) and recovered least after 240 s (11.0% against 47.1%). Across the four materials, recovery tracked the hard-domain melting enthalpy. We attribute the higher fixity and lower recovery primarily to the loss of physical netpoints; a contribution from particle–matrix interactions is possible but could not be separated with the present data. Magnetic actuation was not evaluated in this study. Silane treatments for magnetite-filled TPU should therefore be judged by their effect on hard-segment ordering as well as on dispersion.
SN - 2073-4360
ER -