Salt-Dependent Mechanical and Viscoelastic Deterioration of Epoxy Asphalt Binder Under Repeated Wet-Dry Cycling
- 1School of Highway, Chang’an University, Xi’an 710064, China
- 2Key Laboratory for Special Area Highway Engineering of Ministry of Education, Chang’an University, Xi’an 710064, China
Abstract
Epoxy asphalt (EA) binders are widely used in steel bridge deck pavements because of their high strength and durability. However, their performance deterioration under salt-containing wet-dry conditions, and the differences between chloride and sulfate exposure, remain insufficiently understood. In this study, the deterioration of an EA binder was investigated under wet-dry cycles in pure water, 10 wt% NaCl, and 10 wt% Na2SO4 for up to 16 days. Each cycle comprised immersion at 60 °C for 16 h followed by drying at 60 °C for 8 h. Tensile testing, Shore A hardness measurements, and dynamic mechanical analysis (DMA) were conducted to characterize changes in mechanical properties and temperature-dependent viscoelastic behavior. The results show that after 16 days, tensile strength decreased by 49–56% and elongation at break by 71–78% across the three media. Shore A hardness also declined, with Na2SO4 producing the lowest final value. DMA revealed reductions in storage modulus and glass transition temperature (Tg). The greatest modulus loss at both 25 and 60 °C occurred in the Na2SO4 group, although the temporal deterioration patterns differed between the two temperatures. Tg decreased by 5.26 °C in pure water and by approximately 8.7 °C in both salt solutions. These findings indicate that salt-related deterioration depends on the measured property and test temperature rather than following a single severity ranking. The combined mechanical and viscoelastic results provide a comparative basis for evaluating EA durability under repeated wet-dry salt exposure.
Related
- Viscoelastic Rheology and Constitutive Modeling of Crumb Rubber Modified Asphalt Under Radiation–Low-Temperature Coupled Aging
- Mechanical Reinforcement and Early-Stage Deterioration of Cellulose Nanocrystal-Reinforced Isosorbide-Based Polycarbonate Nanocomposites Under Humid Soil Exposure
- Dynamic Compression Accelerates Degradation-Coupled Mechanical Deterioration of Biomimetic Scaffolds: An In Vitro Platform Study.
- Thermochemical-dependent Cu(i) siting and mobility in Cu-CHA revealed by XAS and quantum mechanical simulations
- Thickness-dependent microstructural transition and mechanical response in thin-walled LPBF-printed Inconel 718 structures
BibTeX
@article{zhang2026saltdependent,
title = {{Salt-Dependent Mechanical and Viscoelastic Deterioration of Epoxy Asphalt Binder Under Repeated Wet-Dry Cycling}},
author = {Yujie Zhang and Aimin Sha and Wenxiu Jiao and Zhuosen Li and Zhanpeng Liu},
journal = {Polymers},
year = {2026},
month = nov,
doi = {10.3390/polym18222912},
url = {https://www.mdpi.com/2073-4360/18/22/2912},
note = {CC BY 4.0},
}
RIS
TY - JOUR
TI - Salt-Dependent Mechanical and Viscoelastic Deterioration of Epoxy Asphalt Binder Under Repeated Wet-Dry Cycling
AU - Yujie Zhang
AU - Aimin Sha
AU - Wenxiu Jiao
AU - Zhuosen Li
AU - Zhanpeng Liu
PY - 2026
DA - 2026/11/19
JO - Polymers
DO - 10.3390/polym18222912
UR - https://www.mdpi.com/2073-4360/18/22/2912
AB - Epoxy asphalt (EA) binders are widely used in steel bridge deck pavements because of their high strength and durability. However, their performance deterioration under salt-containing wet-dry conditions, and the differences between chloride and sulfate exposure, remain insufficiently understood. In this study, the deterioration of an EA binder was investigated under wet-dry cycles in pure water, 10 wt% NaCl, and 10 wt% Na2SO4 for up to 16 days. Each cycle comprised immersion at 60 °C for 16 h followed by drying at 60 °C for 8 h. Tensile testing, Shore A hardness measurements, and dynamic mechanical analysis (DMA) were conducted to characterize changes in mechanical properties and temperature-dependent viscoelastic behavior. The results show that after 16 days, tensile strength decreased by 49–56% and elongation at break by 71–78% across the three media. Shore A hardness also declined, with Na2SO4 producing the lowest final value. DMA revealed reductions in storage modulus and glass transition temperature (Tg). The greatest modulus loss at both 25 and 60 °C occurred in the Na2SO4 group, although the temporal deterioration patterns differed between the two temperatures. Tg decreased by 5.26 °C in pure water and by approximately 8.7 °C in both salt solutions. These findings indicate that salt-related deterioration depends on the measured property and test temperature rather than following a single severity ranking. The combined mechanical and viscoelastic results provide a comparative basis for evaluating EA durability under repeated wet-dry salt exposure.
SN - 2073-4360
ER -