Assessment on work function characterization of thin nanocrystalline silicon layers for silicon heterojunction integration
Abstract
The reported record efficiencies of silicon heterojunction solar cells using hydrogenated nanocrystalline silicon (nc-Si:H) as carrier-collector layers have increased interest in this material due to low activation energy. Band-bending in silicon creates a difference in work function (ϕ) between the bulk and the surface of the film. However, ϕ values of nc-Si:H have only been reported as estimates, with few direct measurements performed. Given the lack of reported data on the ϕ of nc-Si:H films, we compared various measurement techniques to establish reference values and evaluate the reliability of each method. Using Kelvin probe (KP), ultraviolet photoelectron spectroscopy, and electron beam repulsion (EBR), we measured the ϕ of intrinsic, n-type and p-type nc-Si:H layers. We discuss the effect of surface treatments based on ozone and hydrofluoric acid on the ϕ. EBR revealed that the ϕ of p-type films between 10 and 45 nm thick decreases with increasing thickness, dropping from 5.4 to 4.5 eV. This trend was not evident in KP measurements of thinner films. A similar plateau was observed for films thicker than 45 nm by both techniques. We also compared ϕ values measured using these techniques with those estimated from the activation energy obtained via temperature-dependent conductivity measurements.
Related
- Data Characterization and Multi-Plant Data Integration Strategies for Artificial Neural Network Modeling in Palm Oil Refining
- Non-Destructive Mechanical Characterization of 4680 Cylindrical Lithium-Ion Cells for Cell-to-X Integration
- Cascading Valorisation of Agri-Food Waste in Circular Biorefineries: A Critical Review of Technology Integration, Life Cycle Assessment and AI-Assisted Decision Support
- Synthesis of Nanocrystalline Gd2O2NCN from a Versatile Single-source Precursor
- PDBe-SIFTS: An open-source tool for Structure Integration with Function, Taxonomy, and Sequences, featuring improved alignment, scoring scheme, and accelerated search.
BibTeX
@article{leiva2026assessment,
title = {{Assessment on work function characterization of thin nanocrystalline silicon layers for silicon heterojunction integration}},
author = {Amanda Merino Leiva and Pía Vásquez and Sara Zampieri and David Alamarguy and Patricia Martinez and Patricio Häberle and Tristan Gageot and José Alvarez and Jean-Paul Kleider and Valeria del Campo and Delfina Muñoz},
journal = {Solar Energy Materials and Solar Cells},
year = {2026},
month = nov,
doi = {10.1016/j.solmat.2026.114360},
url = {https://hal.science/hal-05607037v1},
note = {CC BY-NC 4.0},
}
RIS
TY - JOUR
TI - Assessment on work function characterization of thin nanocrystalline silicon layers for silicon heterojunction integration
AU - Amanda Merino Leiva
AU - Pía Vásquez
AU - Sara Zampieri
AU - David Alamarguy
AU - Patricia Martinez
AU - Patricio Häberle
AU - Tristan Gageot
AU - José Alvarez
AU - Jean-Paul Kleider
AU - Valeria del Campo
AU - Delfina Muñoz
PY - 2026
DA - 2026/11/17
JO - Solar Energy Materials and Solar Cells
DO - 10.1016/j.solmat.2026.114360
UR - https://hal.science/hal-05607037v1
AB - The reported record efficiencies of silicon heterojunction solar cells using hydrogenated nanocrystalline silicon (nc-Si:H) as carrier-collector layers have increased interest in this material due to low activation energy. Band-bending in silicon creates a difference in work function (ϕ) between the bulk and the surface of the film. However, ϕ values of nc-Si:H have only been reported as estimates, with few direct measurements performed. Given the lack of reported data on the ϕ of nc-Si:H films, we compared various measurement techniques to establish reference values and evaluate the reliability of each method. Using Kelvin probe (KP), ultraviolet photoelectron spectroscopy, and electron beam repulsion (EBR), we measured the ϕ of intrinsic, n-type and p-type nc-Si:H layers. We discuss the effect of surface treatments based on ozone and hydrofluoric acid on the ϕ. EBR revealed that the ϕ of p-type films between 10 and 45 nm thick decreases with increasing thickness, dropping from 5.4 to 4.5 eV. This trend was not evident in KP measurements of thinner films. A similar plateau was observed for films thicker than 45 nm by both techniques. We also compared ϕ values measured using these techniques with those estimated from the activation energy obtained via temperature-dependent conductivity measurements.
SN - 0927-0248
SN - 1879-3398
ER -