Zinc Speciation, Not Total Zinc Loading, Governs Antibacterial Potency and Strain Selectivity in Room-Temperature-Cured Organosiloxane Coatings

7 affiliations
  1. 1Department of Orthopedics, Affiliated Hospital, Guizhou Medical University, Guiyang 550004, China
  2. 2920th Hospital of Joint Logistics Support Force, PLA, Kunming 650032, China
  3. 3School of Clinical Medicine, Dali University, Dali 671000, China
  4. 4Department of Orthopedics, The First People’s Hospital of Zunyi (The Third Affiliated Hospital of Zunyi Medical University), Zunyi 563000, China
  5. 5Pain Department, Qujing City Second People’s Hospital, Qujing 655000, China
  6. 6Department of Orthopedic, The 908th Hospital of Joint Logistic Support Force, Nanchang 330001, China
  7. 7Central South University Institute for Advanced Study, 932 South Lushan Road, Yuelu District, Changsha 410008, China

Abstract

Implant-associated infections call for antimicrobial coatings that combine high efficacy with acceptable cytocompatibility. Here, ZnO nanoparticles (nominal: ~30 nm; 70 ± 40 nm Feret diameter by TEM of the cured film) and Zn2+ ions were co-incorporated into a room-temperature-cured organosiloxane coating at a common nominal total zinc content of 460 ppm (measured by ICP-OES: 554–718 ppm), and the ZnO:Zn2+ molar ratio was varied across five doped formulations (A#–E#) and an undoped control (F#). Antibacterial activity against Escherichia coli (ATCC 25922) and Staphylococcus aureus (ATCC 29213) was measured by the film adhesion method (GB/T 31402) under dark incubation, surface reactive oxygen species (ROS) by DCFH-DA imaging, and cytocompatibility against MC3T3-E1 osteoblasts by CCK-8 (ISO 10993-5). The single-species coatings were complementary rather than equivalent: ZnO-only A# gave 95.05% and 53.36% reductions, and Zn2+-only E# gave 79.32% and 94.66%. The 1:1 formulation C# gave 99.95% and ≥99.60%, exceeding the Bliss-independent additive expectation by 0.97 percentage points for E. coli and by at least 2.09 for S. aureus, and was the only coating whose ROS signal differed significantly from all the others (1.5–2.0× that of A# at half the ZnO-derived zinc). All formulations retained ≥96% osteoblast viability, with no pairwise difference surviving Tukey correction. Neither total zinc content nor mobilized zinc tracked potency, so the ratio—not the dose—controls both activity and strain selectivity. A hypothesis for the interfacial origin of this optimum is stated explicitly as untested.

Related

  1. Tuning Selectivity of Electrochemical Sensors With Polymer Coatings
    Ines C. Weber, Yann Zosso, Diego Uruchurtu Patino +3
    Advanced MaterialsPeer-reviewedLicence not statedFull text6 citedAnalytical chemistryOpenAlex
  2. Carrageenan/epigallocatechin-3-gallate composite hydrogel coatings with antioxidant and antibacterial activities for shrimp preservation
    Linjing Chen, Lei Luo, Lei Qiu +5
    Food Chemistry: XPeer-reviewedCC BY-NC-ND 4.0Full textMaterials & polymersPMC
  3. Antibacterial and Biocompatible Iodine-Releasing Polycationic Coatings Synthesized by Solvent-Free Initiated Chemical Vapor Deposition
    Zihan Xiao, Haijun Gao, Lin Cheng +8
    ACS OmegaPeer-reviewedCC BY-NC-ND 4.0Full textOrganic chemistryCrossrefEurope PMCEurope PMCPMC
  4. 4D-Printed Temperature-Switchable Monolithic Packing for NIR-Actuated Elemental Speciation Analysis.
    Yi-Ting Chen, Yi-Chia Ho, Cheng-Kuan Su
    Analytical chemistryPeer-reviewedCC BYFull textAnalytical chemistryEurope PMC
  5. Microstructure and high-temperature oxidation behaviour of HVOF and plasma sprayed Ni–Cr-based ceramic coatings on SA516 boiler steel
    Ankur Gill, Vikas Chawla, Amit Handa +1
    Results in Surfaces and InterfacesPeer-reviewedCC BYFull textElectrochemistry & energyDOAJ
BibTeX
@article{shao2026zinc,
  title = {{Zinc Speciation, Not Total Zinc Loading, Governs Antibacterial Potency and Strain Selectivity in Room-Temperature-Cured Organosiloxane Coatings}},
  author = {Nengqi Shao and Long Long and Yulei Wang and Di Du and Jinlong Liang and Jiangjun Zhou and Zhijun Cai and Hongkang Zhou and Wenhao Xu and Yongqing Xu and Yi Cui},
  journal = {Molecules},
  year = {2026},
  month = nov,
  doi = {10.3390/molecules31224172},
  url = {https://www.mdpi.com/1420-3049/31/22/4172},
  note = {CC BY 4.0},
}
RIS
TY  - JOUR
TI  - Zinc Speciation, Not Total Zinc Loading, Governs Antibacterial Potency and Strain Selectivity in Room-Temperature-Cured Organosiloxane Coatings
AU  - Nengqi Shao
AU  - Long Long
AU  - Yulei Wang
AU  - Di Du
AU  - Jinlong Liang
AU  - Jiangjun Zhou
AU  - Zhijun Cai
AU  - Hongkang Zhou
AU  - Wenhao Xu
AU  - Yongqing Xu
AU  - Yi Cui
PY  - 2026
DA  - 2026/11/01
JO  - Molecules
DO  - 10.3390/molecules31224172
UR  - https://www.mdpi.com/1420-3049/31/22/4172
AB  - Implant-associated infections call for antimicrobial coatings that combine high efficacy with acceptable cytocompatibility. Here, ZnO nanoparticles (nominal: ~30 nm; 70 ± 40 nm Feret diameter by TEM of the cured film) and Zn2+ ions were co-incorporated into a room-temperature-cured organosiloxane coating at a common nominal total zinc content of 460 ppm (measured by ICP-OES: 554–718 ppm), and the ZnO:Zn2+ molar ratio was varied across five doped formulations (A#–E#) and an undoped control (F#). Antibacterial activity against Escherichia coli (ATCC 25922) and Staphylococcus aureus (ATCC 29213) was measured by the film adhesion method (GB/T 31402) under dark incubation, surface reactive oxygen species (ROS) by DCFH-DA imaging, and cytocompatibility against MC3T3-E1 osteoblasts by CCK-8 (ISO 10993-5). The single-species coatings were complementary rather than equivalent: ZnO-only A# gave 95.05% and 53.36% reductions, and Zn2+-only E# gave 79.32% and 94.66%. The 1:1 formulation C# gave 99.95% and ≥99.60%, exceeding the Bliss-independent additive expectation by 0.97 percentage points for E. coli and by at least 2.09 for S. aureus, and was the only coating whose ROS signal differed significantly from all the others (1.5–2.0× that of A# at half the ZnO-derived zinc). All formulations retained ≥96% osteoblast viability, with no pairwise difference surviving Tukey correction. Neither total zinc content nor mobilized zinc tracked potency, so the ratio—not the dose—controls both activity and strain selectivity. A hypothesis for the interfacial origin of this optimum is stated explicitly as untested.
SN  - 1420-3049