Skip to content
DraconiticResearch
Search Sources API
203,234 studies31 sourcesUpdated 44 min ago
Peer-reviewedCC BY 4.0PLOS One

Study on radiation damage of tungsten-based targets induced by deuterium ions

  1. 1College of Mechanical, Electrical and Aerospace Engineering, Xichang University, Sichuan, China
  2. 2Department of Nuclear Energy, The Engineering and Technical College of Chengdu University of Technology, Sichuan, China
  3. 3School of Mathematics and Physics, Beijing University of Chemical Technology, Beijing, China

Abstract

The effects of homogeneously doped phases on the primary radiation damage of W-based targets were investigated by the Monte Carlo method in this paper. The results show that introducing homogeneously doped phases into W effectively reduces the energy localization of deuterium ions within the targets. Meanwhile, Under 100 keV deuterium ion irradiation, the ballistic distribution, the number of displacement collisions, and the vacancies of deuterium ions in homogeneously doped W targets are all lower than those in pure W. And longitudinal analysis along the depth of all homogeneously doped specimens confirms that homogeneously TiC-doped W offers the strongest suppression of primary radiation damage in the near-surface region. Under 200 keV deuterium ion irradiation, the governing effects of various dopant species and dopant contents on primary radiation damage are summarized as follows: increasing dopant content leads to an approximately linear reduction in vacancies, with Ti dopant showing the strongest vacancy inhibition effect, while the ion range rises linearly and W–TiC possesses the most significant range variation. Large sampling fluctuations of sputtering yield make it an unreliable indicator for evaluating doping performance. Overall, dopants effectively mitigate primary irradiation damage in tungsten. These volume-averaged primary irradiation damage results derived from SRIM simulation are expected to offer reference insights into improving the irradiation tolerance of W by optimizing their compositional design, while microstructural interface effects need further multi-scale modeling for quantitative analysis.

Related

  1. Four Regimes of Primary Radiation Damage in Tungsten
    J. Byggmästar, Ville-Markus Yli-Suutala, Aslak Fellman +3
    Physical Review LettersPeer-reviewedLicence not stated6 citedMaterials & polymersOpenAlex
  2. Thermal expansion of the Martian mineral starkeyite (MgSO4·4H2O) and the effect of synchrotron X-ray radiation damage on its lattice parameters
    Johannes M. Meusburger, Karen A. Hudson-Edwards, Eamonn T. Connolly +2
    ChemRxivPreprintLicence not statedGeneral chemistryChemRxiv
  3. On the radiation damage tolerance of multilayer and single-layer coatings within the ZrN/SiNx system subjected to helium ion implantation
    N. Sénicourt, M.-L. David, K. Mizohata +5
    Surface and Coatings TechnologyPeer-reviewedCC BY1 citedMaterials & polymersCondensed matterHAL
  4. Defect Diamond‐Like d 10 Metal Indium Selenium With Strong Second‐Harmonic Generation and Enhanced Laser‐Induced Damage Threshold
    Muhammad Zeeshan, Zhiyong Bai, Kaijie Xie +7
    SmallPeer-reviewedLicence not statedFull text5 citedMaterials & polymersOpenAlex
  5. Hydrogen Production from Ionizing Radiation-Induced Degradation of Polycarboxylate Ether Polymers La Production d'Hydrogène issue de la Dégradation du PolyCarboxylateEther par les Rayonnements Ionisants
    Vincent Fiegel, Guillaume Blain, Craff Emeline +3
    Comptes Rendus. ChimiePeer-reviewedCC BY 4.0Full textGeneral chemistryHAL
BibTeX
@article{zhang2026study,
  title = {{Study on radiation damage of tungsten-based targets induced by deuterium ions}},
  author = {Yanli Zhang and Fei Zheng and Jiangping Feng and Zhongsheng Cao and Qingyun Meng},
  journal = {PLOS One},
  year = {2026},
  month = oct,
  doi = {10.1371/journal.pone.0360154},
  url = {https://doi.org/10.1371/journal.pone.0360154},
  note = {CC BY 4.0},
}
RIS
TY  - JOUR
TI  - Study on radiation damage of tungsten-based targets induced by deuterium ions
AU  - Yanli Zhang
AU  - Fei Zheng
AU  - Jiangping Feng
AU  - Zhongsheng Cao
AU  - Qingyun Meng
PY  - 2026
DA  - 2026/10/14
JO  - PLOS One
DO  - 10.1371/journal.pone.0360154
UR  - https://doi.org/10.1371/journal.pone.0360154
AB  - The effects of homogeneously doped phases on the primary radiation damage of W-based targets were investigated by the Monte Carlo method in this paper. The results show that introducing homogeneously doped phases into W effectively reduces the energy localization of deuterium ions within the targets. Meanwhile, Under 100 keV deuterium ion irradiation, the ballistic distribution, the number of displacement collisions, and the vacancies of deuterium ions in homogeneously doped W targets are all lower than those in pure W. And longitudinal analysis along the depth of all homogeneously doped specimens confirms that homogeneously TiC-doped W offers the strongest suppression of primary radiation damage in the near-surface region. Under 200 keV deuterium ion irradiation, the governing effects of various dopant species and dopant contents on primary radiation damage are summarized as follows: increasing dopant content leads to an approximately linear reduction in vacancies, with Ti dopant showing the strongest vacancy inhibition effect, while the ion range rises linearly and W–TiC possesses the most significant range variation. Large sampling fluctuations of sputtering yield make it an unreliable indicator for evaluating doping performance. Overall, dopants effectively mitigate primary irradiation damage in tungsten. These volume-averaged primary irradiation damage results derived from SRIM simulation are expected to offer reference insights into improving the irradiation tolerance of W by optimizing their compositional design, while microstructural interface effects need further multi-scale modeling for quantitative analysis.
SN  - 1932-6203
ER  -